Loading ...
Sorry, an error occurred while loading the content.

9231Re: [SCA-JML] Seperate questions about armour

Expand Messages
  • Ash Smith
    Mar 4, 2003
    • 0 Attachment
      Well when I was ordering my plastic I ask around and the general consensus
      was 1/4" ... perhaps I wasn't clear that I was going to be making kozane
      hehe.

      But it's too late now, it's already paid for and partially cut... perhaps I
      should stop while I don't have much of the kozane cut, and do Kiritsuke
      Zane?

      Would actually save me some plastic too... and instead of putting the strips
      of leather/etc, with the plastic I could actually heat and bend it up in
      those portions to zig-zag and (hopefully) do a bit better illusion.

      Ash


      ----- Original Message -----
      From: "Anthony J. Bryant" <ajbryant@...>
      To: <sca-jml@yahoogroups.com>
      Sent: Tuesday, March 04, 2003 7:50 AM
      Subject: Re: [SCA-JML] Seperate questions about armour


      > General comment:
      >
      > <Frank Barone> Holy crap! </Frank Barone>
      >
      > That's .... um..... thick. I wouldn't use anything more than 3/16 for
      kozane,
      > and part of me actually prefers 1/8", given the overlap.
      >
      > Effingham
      >
    • Show all 20 messages in this topic