Loading ...
Sorry, an error occurred while loading the content.

36119Re: [MILL_DRILL] how is that done question

Expand Messages
  • Jerome Kimberlin
    Jul 23, 2014
      On 7/23/2014 1:18 PM, Corey Renner vandal968@... [MILL_DRILL] wrote:
      Broaches do not always go the whole way through.  Rotary broaching is used to make the female hex's on SHCS's and they don't go all the way through.


      It's possible to do it that way, but they don't because it's too slow.  SHCSs are made the usual way - in a cold header.  The hex is just part of the header die sets.

      JerryK
    • Show all 17 messages in this topic