Re: 713 alloy (tenzaloy)

Expand Messages
  • Stankap
    Bret, Look for a local aluminum foundry. I got mine from a foundry near my house in PA, about 30 mi from me. They had ingots, I got 60lb for about $90.00 in
    Message 1 of 2 , Mar 4, 2013
      Bret,
      Look for a local aluminum foundry. I got mine from a foundry near my house in PA, about 30 mi from me. They had ingots, I got 60lb for about $90.00 in 2010.

      I bought it for the same reasons you did, no need for heat treating and it is almost as strong as A356.

      Stan

      --- In hobbicast@yahoogroups.com, "shipmanbb@..." <shipmanbb@...> wrote:
      >
      > Hello, I live near Oklahoma City and was wondering how and where I would go about obtaining tenzaloy? It seems like the perfect thing for me because I need good strength but can't do sophisticated heat treatments.
      >
      > Bret
      >