What is under the silver plating?

Expand Messages
  • ealdredmoneyer
    While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or
    Message 1 of 6 , Feb 22, 2013
    • 0 Attachment
      While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?


      Not a big deal but I am curious.


      Dawson Lewis


      [Non-text portions of this message have been removed]
    • Rupert
      Hello Dawson, See if a magnet sticks to the silverplate you found. If so, it s most likely iron. ... -- yvt Rupert Wenig Camrose, Alberta, Canada. email:
      Message 2 of 6 , Feb 22, 2013
      • 0 Attachment
        Hello Dawson,
        See if a magnet sticks to the silverplate you found. If so, it's
        most likely iron.

        On 2/22/2013 5:02 PM, EaldredSCA@... wrote:
        > While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?
        >
        >
        > Not a big deal but I am curious.
        >
        >
        > Dawson Lewis
        >
        >
        > [Non-text portions of this message have been removed]
        >
        >
        >
        > ------------------------------------
        >
        > For discussion of Metal Casting and related issues
        > this list does not accept attachments.
        >
        > Files area and list services are at:
        > http://groups.yahoo.com/group/hobbicast
        >
        > For additional files and photos and off topic discussions
        > check out these two affiliated sites:
        > http://groups.yahoo.com/group/sandcrabs
        > http://groups.yahoo.com/group/Hobbicast1
        >
        > Please visit our sponsor: Budget Casting Supply
        > http://budgetcastingsupply.com/
        >
        > List Owner:
        > owly@...
        >
        > Yahoo! Groups Links
        >
        >
        >
        >
        >
        > -----
        > No virus found in this message.
        > Checked by AVG - www.avg.com
        > Version: 2013.0.2899 / Virus Database: 2639/6123 - Release Date: 02/22/13
        >
        >

        --

        yvt

        Rupert Wenig
        Camrose, Alberta, Canada.

        email: rwenig2@...

        http://users.xplornet.com/~rwenig/Home/
      • Dan Brewer
        Usually a copper plating and. A steel base. Sent from my iPhone ... [Non-text portions of this message have been removed]
        Message 3 of 6 , Feb 22, 2013
        • 0 Attachment
          Usually a copper plating and. A steel base.

          Sent from my iPhone

          On Feb 22, 2013, at 4:02 PM, EaldredSCA@... wrote:

          > While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?
          >
          > Not a big deal but I am curious.
          >
          > Dawson Lewis
          >
          > [Non-text portions of this message have been removed]
          >
          >


          [Non-text portions of this message have been removed]
        • tmoranwms
          Base could be anything, steel, copper, brass, nickel silver... Only sure way would be to find someone who can do XRF or something like that. Typical plating
          Message 4 of 6 , Feb 22, 2013
          • 0 Attachment
            Base could be anything, steel, copper, brass, nickel silver... Only sure way would be to find someone who can do XRF or something like that.

            Typical plating is a nickel diffusion barrier (prevents silver from "soaking into" the lower layers over time), and the silver plating. I forget if there's more. There may be a copper base plating in there for steel.

            Chrome plating (on steel) is similar, I forget the order of nickel and copper though. I want to say nickel is first, keeping the copper from diffusing into the steel, but nickel and chrome go together well. Ah well, google it. :)

            Tim

            --- In hobbicast@yahoogroups.com, EaldredSCA@... wrote:
            >
            > While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?
            >
            >
            > Not a big deal but I am curious.
            >
            >
            > Dawson Lewis
            >
            >
            > [Non-text portions of this message have been removed]
            >
          • ealdredmoneyer
            Thanks all for the information. Dawson ... From: tmoranwms To: hobbicast Sent: Fri, Feb 22, 2013 7:45 pm
            Message 5 of 6 , Feb 22, 2013
            • 0 Attachment
              Thanks all for the information.


              Dawson



              -----Original Message-----
              From: tmoranwms <tmoranwms@...>
              To: hobbicast <hobbicast@yahoogroups.com>
              Sent: Fri, Feb 22, 2013 7:45 pm
              Subject: [hobbicast] Re: What is under the silver plating?





              Base could be anything, steel, copper, brass, nickel silver... Only sure way would be to find someone who can do XRF or something like that.

              Typical plating is a nickel diffusion barrier (prevents silver from "soaking into" the lower layers over time), and the silver plating. I forget if there's more. There may be a copper base plating in there for steel.

              Chrome plating (on steel) is similar, I forget the order of nickel and copper though. I want to say nickel is first, keeping the copper from diffusing into the steel, but nickel and chrome go together well. Ah well, google it. :)

              Tim

              --- In hobbicast@yahoogroups.com, EaldredSCA@... wrote:
              >
              > While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?
              >
              >
              > Not a big deal but I am curious.
              >
              >
              > Dawson Lewis
              >
              >
              > [Non-text portions of this message have been removed]
              >









              [Non-text portions of this message have been removed]
            • phil
              Hi Dawson, It is usually copper or brass under silver plate, or sometimes a more base metal which has been copper or brass plated before silver plate is
              Message 6 of 6 , Feb 23, 2013
              • 0 Attachment
                Hi Dawson, It is usually copper or brass under silver plate, or sometimes a more base metal which has been copper or brass plated before silver plate is applied.
                Phil
                ----- Original Message -----
                From: EaldredSCA@...
                To: hobbicast@yahoogroups.com
                Sent: Saturday, February 23, 2013 12:02 AM
                Subject: [hobbicast] What is under the silver plating?



                While browsing my local thrift shop I found a couple of silverplated pieces. It got me wondering, what is under the silverplate? Any one ever cut up a piece or melted one down?

                Not a big deal but I am curious.

                Dawson Lewis

                [Non-text portions of this message have been removed]





                [Non-text portions of this message have been removed]
              Your message has been successfully submitted and would be delivered to recipients shortly.