    Rather than pouring the aluminum around the 4 inch tube I would suggest winding it with wire. Stanley Steamer boiler barrels were wound this way and I knew
    Message 1 of 11 , Jan 23 10:13 AM
      Rather than pouring the aluminum around the 4 inch tube I would suggest
      winding it with wire. Stanley Steamer boiler barrels were wound this way
      and I knew someone with a shotgun that had a thin steel barrel wound with
      fibreglass to keep the weight down. This should also eliminate the warping
      of the tube you might get from pouring aluminum around it.

      Stephen C. Lovely

      On Wed, Jan 23, 2013 at 1:42 PM, StoneTool <owly@...> wrote:

      > **
      >
      > 1: The material required to build a 4" cylinder capable of 10,000 PSI
      > is quite expensive and not locally available. I propose to use
      > ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
      > diameter ordinary pipe, say 6", and pour the intervening space full of
      > aluminum.
      >
      >
      >


      [Non-text portions of this message have been removed]
    • StoneTool
      I ve been contemplating a shop press project that is rather unique. The press consists of a set of legs on the floor to support it, and a vertical post, with
      Message 2 of 11 , Jan 23 10:42 AM
        I've been contemplating a shop press project that is rather unique.
        The press consists of a set of legs on the floor to support it, and a
        vertical post, with two parallel channels extending outward toward you,
        and fairly high up. Two frames consisting of a top channel, a pair of
        vertical square tubes, and a bottom tube hang from the two horizontal
        channels that extend from the main post. Each of these frames is half
        of the press frame, and has a channel table that can be raised or
        lowered to the correct height. Because these frames are independent
        and free floating, they can be slid to any spacing or angle desired.
        Clamping bars above the top channels of these frames clamp them firmly
        down to the two channels they hang from so they do not move once
        placed. The two channels these frames hang from have the press cylinder
        attached between them in a fixed location (center).

        Now that the above is clear as mud ;-)........... on to the
        casting portion of the project:

        1: The material required to build a 4" cylinder capable of 10,000 PSI
        is quite expensive and not locally available. I propose to use
        ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
        diameter ordinary pipe, say 6", and pour the intervening space full of
        aluminum


        2: This cylinder will have a ram that passes completely through both
        ends, with the piston in the middle or thereabouts. The problem here
        is that I need to attach a piston capable of transmitting 50 tons to the
        ram. That means either I must use a stepped shaft so the piston has a
        ledge to press on, which means turning the upper portion down and having
        it ground for the high pressure seal, or start with a 4" shaft and turn
        it down, leaving the center portion as the piston............ A LOT of
        material to remove.

        The third option is to take a 1.5" shaft, and turn a groove into it
        to accept a heavy snap ring or something of the sort, and simply pour
        the ram right on the shaft. This of course means designing the mold so
        I can turn out a pocket in the aluminum ram to accept a pressure seal or
        just a high pressure O-ring. No big deal.


        Option3 appeals to me.............. any thoughts?

        * Now to the why of it. The first part, the press design is pretty
        obvious, but the ram design may not be as obvious to some. Here are the
        reasons.

        1: Keeping the spacing between the support points constant as the
        cylinder extends. That is to say that with an ordinary cylinder, as the
        ram approaches the end bushing any play is magnified. If you have a
        couple thousandths of an inch at the top of the stroke, there will be
        quite a bit by the time it is extended.

        2: Impact......... I want a press where I can have an impact weight on
        top....... lifted by air and dropped, and transmit that impact all the
        way down through the ram. With impact, you can move something at 10
        tons that would otherwise take the full 50 tons....... and not break it.


        I would draw up a sketch, but I'm not much of a draftsman........ I
        know what I want, and have a very clear picture in my head of
        it............ enough to build it. I tend to do things that way.


        Howard
      • Allen Powell
        Stone Tool, Are going to be pressurizing your cylinder to 10,000 PSI? You ll need that if your going to be using a 4 bore cylinder with a 1 1/2 rod. Are you
        Message 3 of 11 , Jan 23 12:41 PM
          Stone Tool,

          Are going to be pressurizing your cylinder to 10,000 PSI? You'll need that
          if your going to be using a 4" bore cylinder with a 1 1/2" rod. Are you
          using a hand pump? What is the cylinder stroke? What will pump
          displacement be and how fast do you expect the the rod to travel full
          stroke? Double or single acting? What will you be using for a valve?

          Check this site out:
          http://www.tksimplex.com/customfiles/R%20SERIES.pdf

          http://www.tksimplex.com/html/product_detail.php?pid=295&catname=Hydraulic%20Steel%20Cylinders&scatname=Spring%20Return%20%28R%20Series%29

          Not trying yo dissuade you, but...

          Al


          On Wed, Jan 23, 2013 at 1:43 PM, StoneTool <owly@...> wrote:

          > **
          >
          >
          > Good Thought Stephen:
          >
          > .........I would need to be wound under a lot of tension to do any
          > good. If not the tube would still expand losing the dimension for the
          > seal.
          >
          > I've also thought of using sand lightly coated with epoxy resin and
          > put packed in under pressure with a hydraulic press.
          >
          > The distortion issue is one that bothered me somewhat, as I have no
          > idea how much distortion one would get. The outer pipe could poured
          > full of aluminum with a core so once the core was knocked out, it could
          > be easily machined for a press fit also. That would eliminate the
          > distortion issue.
          >
          > In the same vein, I could make a pair of clips out of steel similar
          > to what are used to hold axles into a Chevy rear axle....just two half
          > rounds, fairly thick, machine a groove in the ram to match them, and
          > machine a piece of steel that was a fairly tight fit around the ram....
          > one you have to heat to slip it on, with a pocket that matched the
          > clips. Slip the piece down over the clips, and weld the clips into the
          > piece, giving myself a fairly large diameter flange around the ram which
          > the aluminum piston could slide down against and be attached with a
          > couple of small screws. A four piece arrangement..........
          >
          > Howard
          >
          > On 01/23/2013 11:13 AM, Stephen Lovely wrote:
          > > Rather than pouring the aluminum around the 4 inch tube I would suggest
          > > winding it with wire. Stanley Steamer boiler barrels were wound this way
          > > and I knew someone with a shotgun that had a thin steel barrel wound with
          > > fibreglass to keep the weight down. This should also eliminate the
          > warping
          > > of the tube you might get from pouring aluminum around it.
          > >
          > > Stephen C. Lovely
          > >
          > > On Wed, Jan 23, 2013 at 1:42 PM, StoneToolowly@...> wrote:
          > >
          > >> **
          > >>
          > >> 1: The material required to build a 4" cylinder capable of 10,000 PSI
          > >> is quite expensive and not locally available. I propose to use
          > >> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
          > >> diameter ordinary pipe, say 6", and pour the intervening space full of
          > >> aluminum.
          > >>
          > >>
          > >>
          > >
          > > [Non-text portions of this message have been removed]
          > >
          > >
          > >
          > > ------------------------------------
          > >
          > > For discussion of Metal Casting and related issues
          > > this list does not accept attachments.
          > >
          > > Files area and list services are at:
          > > http://groups.yahoo.com/group/hobbicast
          > >
          > > For additional files and photos and off topic discussions
          > > check out these two affiliated sites:
          > > http://groups.yahoo.com/group/sandcrabs
          > > http://groups.yahoo.com/group/Hobbicast1
          > >
          > > Please visit our sponsor: Budget Casting Supply
          > > http://budgetcastingsupply.com/
          > >
          > > List Owner:
          > > owly@...
          > >
          > > Yahoo! Groups Links
          > >
          > >
          > >
          > >
          >
          >
          >


          [Non-text portions of this message have been removed]
        • StoneTool
          Good Thought Stephen: .........I would need to be wound under a lot of tension to do any good. If not the tube would still expand losing the dimension for the
          Message 4 of 11 , Jan 23 12:43 PM
            Good Thought Stephen:

            .........I would need to be wound under a lot of tension to do any
            good. If not the tube would still expand losing the dimension for the
            seal.

            I've also thought of using sand lightly coated with epoxy resin and
            put packed in under pressure with a hydraulic press.

            The distortion issue is one that bothered me somewhat, as I have no
            idea how much distortion one would get. The outer pipe could poured
            full of aluminum with a core so once the core was knocked out, it could
            be easily machined for a press fit also. That would eliminate the
            distortion issue.

            In the same vein, I could make a pair of clips out of steel similar
            to what are used to hold axles into a Chevy rear axle....just two half
            rounds, fairly thick, machine a groove in the ram to match them, and
            machine a piece of steel that was a fairly tight fit around the ram....
            one you have to heat to slip it on, with a pocket that matched the
            clips. Slip the piece down over the clips, and weld the clips into the
            piece, giving myself a fairly large diameter flange around the ram which
            the aluminum piston could slide down against and be attached with a
            couple of small screws. A four piece arrangement..........

            Howard



            On 01/23/2013 11:13 AM, Stephen Lovely wrote:
            > Rather than pouring the aluminum around the 4 inch tube I would suggest
            > winding it with wire. Stanley Steamer boiler barrels were wound this way
            > and I knew someone with a shotgun that had a thin steel barrel wound with
            > fibreglass to keep the weight down. This should also eliminate the warping
            > of the tube you might get from pouring aluminum around it.
            >
            > Stephen C. Lovely
            >
            > On Wed, Jan 23, 2013 at 1:42 PM, StoneTool<owly@...> wrote:
            >
            >> **
            >>
            >> 1: The material required to build a 4" cylinder capable of 10,000 PSI
            >> is quite expensive and not locally available. I propose to use
            >> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
            >> diameter ordinary pipe, say 6", and pour the intervening space full of
            >> aluminum.
            >>
            >>
            >>
            >
            > [Non-text portions of this message have been removed]
            >
            >
            >
            > ------------------------------------
            >
            > For discussion of Metal Casting and related issues
            > this list does not accept attachments.
            >
            > Files area and list services are at:
            > http://groups.yahoo.com/group/hobbicast
            >
            > For additional files and photos and off topic discussions
            > check out these two affiliated sites:
            > http://groups.yahoo.com/group/sandcrabs
            > http://groups.yahoo.com/group/Hobbicast1
            >
            > Please visit our sponsor: Budget Casting Supply
            > http://budgetcastingsupply.com/
            >
            > List Owner:
            > owly@...
            >
            > Yahoo! Groups Links
            >
            >
            >
            >
          • redlupmi2
            I ll share my experience. I don t think an aluminum piston will transmit that much pressure to a 1-1/2 steel rod, without deforming. Besides the columnar
            Message 5 of 11 , Jan 23 4:46 PM
              I'll share my experience.

              I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.

              My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.

              The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.

              Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.

              4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.

              As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.

              Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.

              If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.

              Plan carefully, and work safely.

              R.T. :D

              --- In hobbicast@yahoogroups.com, StoneTool wrote:
              >
              > I've been contemplating a shop press project that is rather unique.
              > The press consists of a set of legs on the floor to support it, and a
              > vertical post, with two parallel channels extending outward toward you,
              > and fairly high up. Two frames consisting of a top channel, a pair of
              > vertical square tubes, and a bottom tube hang from the two horizontal
              > channels that extend from the main post. Each of these frames is half
              > of the press frame, and has a channel table that can be raised or
              > lowered to the correct height. Because these frames are independent
              > and free floating, they can be slid to any spacing or angle desired.
              > Clamping bars above the top channels of these frames clamp them firmly
              > down to the two channels they hang from so they do not move once
              > placed. The two channels these frames hang from have the press cylinder
              > attached between them in a fixed location (center).
              >
              > Now that the above is clear as mud ;-)........... on to the
              > casting portion of the project:
              >
              > 1: The material required to build a 4" cylinder capable of 10,000 PSI
              > is quite expensive and not locally available. I propose to use
              > ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
              > diameter ordinary pipe, say 6", and pour the intervening space full of
              > aluminum
              >
              >
              > 2: This cylinder will have a ram that passes completely through both
              > ends, with the piston in the middle or thereabouts. The problem here
              > is that I need to attach a piston capable of transmitting 50 tons to the
              > ram. That means either I must use a stepped shaft so the piston has a
              > ledge to press on, which means turning the upper portion down and having
              > it ground for the high pressure seal, or start with a 4" shaft and turn
              > it down, leaving the center portion as the piston............ A LOT of
              > material to remove.
              >
              > The third option is to take a 1.5" shaft, and turn a groove into it
              > to accept a heavy snap ring or something of the sort, and simply pour
              > the ram right on the shaft. This of course means designing the mold so
              > I can turn out a pocket in the aluminum ram to accept a pressure seal or
              > just a high pressure O-ring. No big deal.
              >
              >
              > Option3 appeals to me.............. any thoughts?
              >
              > * Now to the why of it. The first part, the press design is pretty
              > obvious, but the ram design may not be as obvious to some. Here are the
              > reasons.
              >
              > 1: Keeping the spacing between the support points constant as the
              > cylinder extends. That is to say that with an ordinary cylinder, as the
              > ram approaches the end bushing any play is magnified. If you have a
              > couple thousandths of an inch at the top of the stroke, there will be
              > quite a bit by the time it is extended.
              >
              > 2: Impact......... I want a press where I can have an impact weight on
              > top....... lifted by air and dropped, and transmit that impact all the
              > way down through the ram. With impact, you can move something at 10
              > tons that would otherwise take the full 50 tons....... and not break it.
              >
              >
              > I would draw up a sketch, but I'm not much of a draftsman........ I
              > know what I want, and have a very clear picture in my head of
              > it............ enough to build it. I tend to do things that way.
              >
              >
              > Howard
              >
            • StoneTool
              Allen: You surmised correctly........... I have an electric pump that pushes 10K that I use with my other 50 ton rams. The stroke will probably be about
              Message 6 of 11 , Jan 23 9:07 PM
                Allen:
                You surmised correctly........... I have an electric pump that
                pushes 10K that I use with my other 50 ton rams. The stroke will
                probably be about 12". That would give me about 130 cubic inches.
                Travel speed is irrelevant. Presses move pretty slow....... as they
                should. I've never hooked my flow meter up to this pump, but volume is
                quite low. This cylinder will be single acting (hydraulic), with
                compressed air to return it. I use a gate valve rated for 10K right at
                the pump.

                I'm contemplating building a special pumping system that uses a 1
                HP motor driving an ordinary hydraulic cylinder at normal pressures.
                Around 2500 PSI, and a special cylinder with a ram sized so pressure on
                one end will step up pressure on the other end 4x by virtue of ram
                size. The idea being that there would be fast travel (4x), and once
                pressure rose to 2500, oil would be diverted to the special cylinder
                which would then output 10K at 1/4 volume.
                I've planned this system out in some detail a number of times......
                an elegant way to get speed for low pressure jobs and pressure for the
                heavy pressing jobs. I don't think I'll do it right now....... the
                basic press design is what I'm working on.


                Howard



                On 01/23/2013 01:41 PM, Allen Powell wrote:
                > Stone Tool,
                >
                > Are going to be pressurizing your cylinder to 10,000 PSI? You'll need that
                > if your going to be using a 4" bore cylinder with a 1 1/2" rod. Are you
                > using a hand pump? What is the cylinder stroke? What will pump
                > displacement be and how fast do you expect the the rod to travel full
                > stroke? Double or single acting? What will you be using for a valve?
                >
                > Check this site out:
                > http://www.tksimplex.com/customfiles/R%20SERIES.pdf
                >
                > http://www.tksimplex.com/html/product_detail.php?pid=295&catname=Hydraulic%20Steel%20Cylinders&scatname=Spring%20Return%20%28R%20Series%29
                >
                > Not trying yo dissuade you, but...
                >
                > Al
                >
                >
                > On Wed, Jan 23, 2013 at 1:43 PM, StoneTool<owly@...> wrote:
                >
                >> **
                >>
                >>
                >> Good Thought Stephen:
                >>
                >> .........I would need to be wound under a lot of tension to do any
                >> good. If not the tube would still expand losing the dimension for the
                >> seal.
                >>
                >> I've also thought of using sand lightly coated with epoxy resin and
                >> put packed in under pressure with a hydraulic press.
                >>
                >> The distortion issue is one that bothered me somewhat, as I have no
                >> idea how much distortion one would get. The outer pipe could poured
                >> full of aluminum with a core so once the core was knocked out, it could
                >> be easily machined for a press fit also. That would eliminate the
                >> distortion issue.
                >>
                >> In the same vein, I could make a pair of clips out of steel similar
                >> to what are used to hold axles into a Chevy rear axle....just two half
                >> rounds, fairly thick, machine a groove in the ram to match them, and
                >> machine a piece of steel that was a fairly tight fit around the ram....
                >> one you have to heat to slip it on, with a pocket that matched the
                >> clips. Slip the piece down over the clips, and weld the clips into the
                >> piece, giving myself a fairly large diameter flange around the ram which
                >> the aluminum piston could slide down against and be attached with a
                >> couple of small screws. A four piece arrangement..........
                >>
                >> Howard
                >>
                >> On 01/23/2013 11:13 AM, Stephen Lovely wrote:
                >>> Rather than pouring the aluminum around the 4 inch tube I would suggest
                >>> winding it with wire. Stanley Steamer boiler barrels were wound this way
                >>> and I knew someone with a shotgun that had a thin steel barrel wound with
                >>> fibreglass to keep the weight down. This should also eliminate the
                >> warping
                >>> of the tube you might get from pouring aluminum around it.
                >>>
                >>> Stephen C. Lovely
                >>>
                >>> On Wed, Jan 23, 2013 at 1:42 PM, StoneToolowly@...> wrote:
                >>>
                >>>> **
                >>>>
                >>>> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                >>>> is quite expensive and not locally available. I propose to use
                >>>> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                >>>> diameter ordinary pipe, say 6", and pour the intervening space full of
                >>>> aluminum.
                >>>>
                >>>>
                >>>>
                >>> [Non-text portions of this message have been removed]
                >>>
                >>>
                >>>
                >>> ------------------------------------
                >>>
                >>> For discussion of Metal Casting and related issues
                >>> this list does not accept attachments.
                >>>
                >>> Files area and list services are at:
                >>> http://groups.yahoo.com/group/hobbicast
                >>>
                >>> For additional files and photos and off topic discussions
                >>> check out these two affiliated sites:
                >>> http://groups.yahoo.com/group/sandcrabs
                >>> http://groups.yahoo.com/group/Hobbicast1
                >>>
                >>> Please visit our sponsor: Budget Casting Supply
                >>> http://budgetcastingsupply.com/
                >>>
                >>> List Owner:
                >>> owly@...
                >>>
                >>> Yahoo! Groups Links
                >>>
                >>>
                >>>
                >>>
                >>
                >>
                >
                > [Non-text portions of this message have been removed]
                >
                >
                >
                > ------------------------------------
                >
                > For discussion of Metal Casting and related issues
                > this list does not accept attachments.
                >
                > Files area and list services are at:
                > http://groups.yahoo.com/group/hobbicast
                >
                > For additional files and photos and off topic discussions
                > check out these two affiliated sites:
                > http://groups.yahoo.com/group/sandcrabs
                > http://groups.yahoo.com/group/Hobbicast1
                >
                > Please visit our sponsor: Budget Casting Supply
                > http://budgetcastingsupply.com/
                >
                > List Owner:
                > owly@...
                >
                > Yahoo! Groups Links
                >
                >
                >
                >
              • StoneTool
                RT: Thanks for the share............ I work with 50 ton stuff all the time I agree that an aluminum piston will not transmit 50 T to a 1.5 rod without
                Message 7 of 11 , Jan 23 9:31 PM
                  RT:
                  Thanks for the share............

                  I work with 50 ton stuff all the time

                  I agree that an aluminum piston will not transmit 50 T to a
                  1.5" rod without deforming unless there is steel to spread the force out
                  wider. I like an Aluminum piston because of wear. I've seen too many
                  steel pistons gall cylinders when the wear bands don't quite do the
                  job. In addition seals for that kind of pressure must run at VERY close
                  tolerance. I don't like steel on steel when tolerances are very
                  close. Cast iron on steel works well, as does brass or aluminum.
                  I share your concerns about things blowing out of presses to the
                  extent that I once built a press based on a 1" thick steel table with
                  various openings, and the press portion moved up and down so your
                  working height was always the table top. The idea was to weld support
                  structures right to the table for pressing so everything was rigid.
                  It's a good machine and still in service. A 12" centrally located round
                  hole with a flange beneath it for reinforcement is the primary work
                  area, and press blocks of 1" plate are used to bridge the hole. It also
                  has a slot 8" wide and a number of other holes, and the cylinder can be
                  located at virtually any point on the surface. It uses a 50 ton
                  Owatanna porta power cylinder and electric pump. A rather unique and
                  elegant system that cost a lot of money by the time I was done...... I
                  don't own it and couldn't afford to build one like it for my own use.
                  Threaded rods across between the table sections may be needed on
                  the press I'm contemplating to maintain their relationship, though I'm
                  looking at other and more convenient means of securing them. Top
                  clamping alone is probably not enough. I've examined a lot of
                  different ways of doing things from top and bottom eccentric clamping to
                  hydraulic clamping with press pressure, to half nuts to other positive
                  dogging methods. I haven't nailed down a final design yet.


                  Howard

                  On 01/23/2013 05:46 PM, redlupmi2 wrote:
                  > I'll share my experience.
                  >
                  > I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.
                  >
                  > My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.
                  >
                  > The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.
                  >
                  > Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.
                  >
                  > 4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.
                  >
                  > As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.
                  >
                  > Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.
                  >
                  > If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.
                  >
                  > Plan carefully, and work safely.
                  >
                  > R.T. :D
                  >
                  > --- In hobbicast@yahoogroups.com, StoneTool wrote:
                  >> I've been contemplating a shop press project that is rather unique.
                  >> The press consists of a set of legs on the floor to support it, and a
                  >> vertical post, with two parallel channels extending outward toward you,
                  >> and fairly high up. Two frames consisting of a top channel, a pair of
                  >> vertical square tubes, and a bottom tube hang from the two horizontal
                  >> channels that extend from the main post. Each of these frames is half
                  >> of the press frame, and has a channel table that can be raised or
                  >> lowered to the correct height. Because these frames are independent
                  >> and free floating, they can be slid to any spacing or angle desired.
                  >> Clamping bars above the top channels of these frames clamp them firmly
                  >> down to the two channels they hang from so they do not move once
                  >> placed. The two channels these frames hang from have the press cylinder
                  >> attached between them in a fixed location (center).
                  >>
                  >> Now that the above is clear as mud ;-)........... on to the
                  >> casting portion of the project:
                  >>
                  >> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                  >> is quite expensive and not locally available. I propose to use
                  >> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                  >> diameter ordinary pipe, say 6", and pour the intervening space full of
                  >> aluminum
                  >>
                  >>
                  >> 2: This cylinder will have a ram that passes completely through both
                  >> ends, with the piston in the middle or thereabouts. The problem here
                  >> is that I need to attach a piston capable of transmitting 50 tons to the
                  >> ram. That means either I must use a stepped shaft so the piston has a
                  >> ledge to press on, which means turning the upper portion down and having
                  >> it ground for the high pressure seal, or start with a 4" shaft and turn
                  >> it down, leaving the center portion as the piston............ A LOT of
                  >> material to remove.
                  >>
                  >> The third option is to take a 1.5" shaft, and turn a groove into it
                  >> to accept a heavy snap ring or something of the sort, and simply pour
                  >> the ram right on the shaft. This of course means designing the mold so
                  >> I can turn out a pocket in the aluminum ram to accept a pressure seal or
                  >> just a high pressure O-ring. No big deal.
                  >>
                  >>
                  >> Option3 appeals to me.............. any thoughts?
                  >>
                  >> * Now to the why of it. The first part, the press design is pretty
                  >> obvious, but the ram design may not be as obvious to some. Here are the
                  >> reasons.
                  >>
                  >> 1: Keeping the spacing between the support points constant as the
                  >> cylinder extends. That is to say that with an ordinary cylinder, as the
                  >> ram approaches the end bushing any play is magnified. If you have a
                  >> couple thousandths of an inch at the top of the stroke, there will be
                  >> quite a bit by the time it is extended.
                  >>
                  >> 2: Impact......... I want a press where I can have an impact weight on
                  >> top....... lifted by air and dropped, and transmit that impact all the
                  >> way down through the ram. With impact, you can move something at 10
                  >> tons that would otherwise take the full 50 tons....... and not break it.
                  >>
                  >>
                  >> I would draw up a sketch, but I'm not much of a draftsman........ I
                  >> know what I want, and have a very clear picture in my head of
                  >> it............ enough to build it. I tend to do things that way.
                  >>
                  >>
                  >> Howard
                  >>
                  >
                  >
                  >
                  > ------------------------------------
                  >
                  > For discussion of Metal Casting and related issues
                  > this list does not accept attachments.
                  >
                  > Files area and list services are at:
                  > http://groups.yahoo.com/group/hobbicast
                  >
                  > For additional files and photos and off topic discussions
                  > check out these two affiliated sites:
                  > http://groups.yahoo.com/group/sandcrabs
                  > http://groups.yahoo.com/group/Hobbicast1
                  >
                  > Please visit our sponsor: Budget Casting Supply
                  > http://budgetcastingsupply.com/
                  >
                  > List Owner:
                  > owly@...
                  >
                  > Yahoo! Groups Links
                  >
                  >
                  >
                  >
                • redlupmi2
                  Glad to know you have experience with 50 ton presses. Some pay a high price for the experience. A local hydraulic cylinder builder takes a steel piston and
                  Message 8 of 11 , Jan 24 2:23 PM
                    Glad to know you have experience with 50 ton presses. Some pay a high price for the experience.

                    A local hydraulic cylinder builder takes a steel piston and brazes a layer of brass or welds a layer of silicon bronze to the OD of some of their pistons then machines to finish size.

                    R.T. :D

                    --- In hobbicast@yahoogroups.com, StoneTool wrote:
                    >
                    > RT:
                    > Thanks for the share............
                    >
                    > I work with 50 ton stuff all the time
                    >
                    > I agree that an aluminum piston will not transmit 50 T to a
                    > 1.5" rod without deforming unless there is steel to spread the force out
                    > wider. I like an Aluminum piston because of wear. I've seen too many
                    > steel pistons gall cylinders when the wear bands don't quite do the
                    > job. In addition seals for that kind of pressure must run at VERY close
                    > tolerance. I don't like steel on steel when tolerances are very
                    > close. Cast iron on steel works well, as does brass or aluminum.
                    > I share your concerns about things blowing out of presses to the
                    > extent that I once built a press based on a 1" thick steel table with
                    > various openings, and the press portion moved up and down so your
                    > working height was always the table top. The idea was to weld support
                    > structures right to the table for pressing so everything was rigid.
                    > It's a good machine and still in service. A 12" centrally located round
                    > hole with a flange beneath it for reinforcement is the primary work
                    > area, and press blocks of 1" plate are used to bridge the hole. It also
                    > has a slot 8" wide and a number of other holes, and the cylinder can be
                    > located at virtually any point on the surface. It uses a 50 ton
                    > Owatanna porta power cylinder and electric pump. A rather unique and
                    > elegant system that cost a lot of money by the time I was done...... I
                    > don't own it and couldn't afford to build one like it for my own use.
                    > Threaded rods across between the table sections may be needed on
                    > the press I'm contemplating to maintain their relationship, though I'm
                    > looking at other and more convenient means of securing them. Top
                    > clamping alone is probably not enough. I've examined a lot of
                    > different ways of doing things from top and bottom eccentric clamping to
                    > hydraulic clamping with press pressure, to half nuts to other positive
                    > dogging methods. I haven't nailed down a final design yet.
                    >
                    >
                    > Howard
                    >
                    > On 01/23/2013 05:46 PM, redlupmi2 wrote:
                    > > I'll share my experience.
                    > >
                    > > I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.
                    > >
                    > > My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.
                    > >
                    > > The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.
                    > >
                    > > Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.
                    > >
                    > > 4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.
                    > >
                    > > As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.
                    > >
                    > > Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.
                    > >
                    > > If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.
                    > >
                    > > Plan carefully, and work safely.
                    > >
                    > > R.T. :D
                    > >
                    > > --- In hobbicast@yahoogroups.com, StoneTool wrote:
                    > >> I've been contemplating a shop press project that is rather unique.
                    > >> The press consists of a set of legs on the floor to support it, and a
                    > >> vertical post, with two parallel channels extending outward toward you,
                    > >> and fairly high up. Two frames consisting of a top channel, a pair of
                    > >> vertical square tubes, and a bottom tube hang from the two horizontal
                    > >> channels that extend from the main post. Each of these frames is half
                    > >> of the press frame, and has a channel table that can be raised or
                    > >> lowered to the correct height. Because these frames are independent
                    > >> and free floating, they can be slid to any spacing or angle desired.
                    > >> Clamping bars above the top channels of these frames clamp them firmly
                    > >> down to the two channels they hang from so they do not move once
                    > >> placed. The two channels these frames hang from have the press cylinder
                    > >> attached between them in a fixed location (center).
                    > >>
                    > >> Now that the above is clear as mud ;-)........... on to the
                    > >> casting portion of the project:
                    > >>
                    > >> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                    > >> is quite expensive and not locally available. I propose to use
                    > >> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                    > >> diameter ordinary pipe, say 6", and pour the intervening space full of
                    > >> aluminum
                    > >>
                    > >>
                    > >> 2: This cylinder will have a ram that passes completely through both
                    > >> ends, with the piston in the middle or thereabouts. The problem here
                    > >> is that I need to attach a piston capable of transmitting 50 tons to the
                    > >> ram. That means either I must use a stepped shaft so the piston has a
                    > >> ledge to press on, which means turning the upper portion down and having
                    > >> it ground for the high pressure seal, or start with a 4" shaft and turn
                    > >> it down, leaving the center portion as the piston............ A LOT of
                    > >> material to remove.
                    > >>
                    > >> The third option is to take a 1.5" shaft, and turn a groove into it
                    > >> to accept a heavy snap ring or something of the sort, and simply pour
                    > >> the ram right on the shaft. This of course means designing the mold so
                    > >> I can turn out a pocket in the aluminum ram to accept a pressure seal or
                    > >> just a high pressure O-ring. No big deal.
                    > >>
                    > >>
                    > >> Option3 appeals to me.............. any thoughts?
                    > >>
                    > >> * Now to the why of it. The first part, the press design is pretty
                    > >> obvious, but the ram design may not be as obvious to some. Here are the
                    > >> reasons.
                    > >>
                    > >> 1: Keeping the spacing between the support points constant as the
                    > >> cylinder extends. That is to say that with an ordinary cylinder, as the
                    > >> ram approaches the end bushing any play is magnified. If you have a
                    > >> couple thousandths of an inch at the top of the stroke, there will be
                    > >> quite a bit by the time it is extended.
                    > >>
                    > >> 2: Impact......... I want a press where I can have an impact weight on
                    > >> top....... lifted by air and dropped, and transmit that impact all the
                    > >> way down through the ram. With impact, you can move something at 10
                    > >> tons that would otherwise take the full 50 tons....... and not break it.
                    > >>
                    > >>
                    > >> I would draw up a sketch, but I'm not much of a draftsman........ I
                    > >> know what I want, and have a very clear picture in my head of
                    > >> it............ enough to build it. I tend to do things that way.
                    > >>
                    > >>
                    > >> Howard
                    > >>
                    > >
                    > >
                    > >
                    > > ------------------------------------
                    > >
                    > > For discussion of Metal Casting and related issues
                    > > this list does not accept attachments.
                    > >
                    > > Files area and list services are at:
                    > > http://groups.yahoo.com/group/hobbicast
                    > >
                    > > For additional files and photos and off topic discussions
                    > > check out these two affiliated sites:
                    > > http://groups.yahoo.com/group/sandcrabs
                    > > http://groups.yahoo.com/group/Hobbicast1
                    > >
                    > > Please visit our sponsor: Budget Casting Supply
                    > > http://budgetcastingsupply.com/
                    > >
                    > > List Owner:
                    > > owly@...
                    > >
                    > > Yahoo! Groups Links
                    > >
                    > >
                    > >
                    > >
                    >
                  • StoneTool
                    I have a 50 ton ram with 8 stroke that has a solid brass ram & piston............ Howard
                    Message 9 of 11 , Jan 24 7:51 PM
                      I have a 50 ton ram with 8" stroke that has a solid brass ram &
                      piston............


                      Howard

                      On 01/24/2013 03:23 PM, redlupmi2 wrote:
                      > Glad to know you have experience with 50 ton presses. Some pay a high price for the experience.
                      >
                      > A local hydraulic cylinder builder takes a steel piston and brazes a layer of brass or welds a layer of silicon bronze to the OD of some of their pistons then machines to finish size.
                      >
                      > R.T. :D
                      >
                      > --- In hobbicast@yahoogroups.com, StoneTool wrote:
                      >> RT:
                      >> Thanks for the share............
                      >>
                      >> I work with 50 ton stuff all the time
                      >>
                      >> I agree that an aluminum piston will not transmit 50 T to a
                      >> 1.5" rod without deforming unless there is steel to spread the force out
                      >> wider. I like an Aluminum piston because of wear. I've seen too many
                      >> steel pistons gall cylinders when the wear bands don't quite do the
                      >> job. In addition seals for that kind of pressure must run at VERY close
                      >> tolerance. I don't like steel on steel when tolerances are very
                      >> close. Cast iron on steel works well, as does brass or aluminum.
                      >> I share your concerns about things blowing out of presses to the
                      >> extent that I once built a press based on a 1" thick steel table with
                      >> various openings, and the press portion moved up and down so your
                      >> working height was always the table top. The idea was to weld support
                      >> structures right to the table for pressing so everything was rigid.
                      >> It's a good machine and still in service. A 12" centrally located round
                      >> hole with a flange beneath it for reinforcement is the primary work
                      >> area, and press blocks of 1" plate are used to bridge the hole. It also
                      >> has a slot 8" wide and a number of other holes, and the cylinder can be
                      >> located at virtually any point on the surface. It uses a 50 ton
                      >> Owatanna porta power cylinder and electric pump. A rather unique and
                      >> elegant system that cost a lot of money by the time I was done...... I
                      >> don't own it and couldn't afford to build one like it for my own use.
                      >> Threaded rods across between the table sections may be needed on
                      >> the press I'm contemplating to maintain their relationship, though I'm
                      >> looking at other and more convenient means of securing them. Top
                      >> clamping alone is probably not enough. I've examined a lot of
                      >> different ways of doing things from top and bottom eccentric clamping to
                      >> hydraulic clamping with press pressure, to half nuts to other positive
                      >> dogging methods. I haven't nailed down a final design yet.
                      >>
                      >>
                      >> Howard
                      >>
                      >> On 01/23/2013 05:46 PM, redlupmi2 wrote:
                      >>> I'll share my experience.
                      >>>
                      >>> I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.
                      >>>
                      >>> My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.
                      >>>
                      >>> The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.
                      >>>
                      >>> Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.
                      >>>
                      >>> 4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.
                      >>>
                      >>> As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.
                      >>>
                      >>> Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.
                      >>>
                      >>> If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.
                      >>>
                      >>> Plan carefully, and work safely.
                      >>>
                      >>> R.T. :D
                      >>>
                      >>> --- In hobbicast@yahoogroups.com, StoneTool wrote:
                      >>>> I've been contemplating a shop press project that is rather unique.
                      >>>> The press consists of a set of legs on the floor to support it, and a
                      >>>> vertical post, with two parallel channels extending outward toward you,
                      >>>> and fairly high up. Two frames consisting of a top channel, a pair of
                      >>>> vertical square tubes, and a bottom tube hang from the two horizontal
                      >>>> channels that extend from the main post. Each of these frames is half
                      >>>> of the press frame, and has a channel table that can be raised or
                      >>>> lowered to the correct height. Because these frames are independent
                      >>>> and free floating, they can be slid to any spacing or angle desired.
                      >>>> Clamping bars above the top channels of these frames clamp them firmly
                      >>>> down to the two channels they hang from so they do not move once
                      >>>> placed. The two channels these frames hang from have the press cylinder
                      >>>> attached between them in a fixed location (center).
                      >>>>
                      >>>> Now that the above is clear as mud ;-)........... on to the
                      >>>> casting portion of the project:
                      >>>>
                      >>>> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                      >>>> is quite expensive and not locally available. I propose to use
                      >>>> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                      >>>> diameter ordinary pipe, say 6", and pour the intervening space full of
                      >>>> aluminum
                      >>>>
                      >>>>
                      >>>> 2: This cylinder will have a ram that passes completely through both
                      >>>> ends, with the piston in the middle or thereabouts. The problem here
                      >>>> is that I need to attach a piston capable of transmitting 50 tons to the
                      >>>> ram. That means either I must use a stepped shaft so the piston has a
                      >>>> ledge to press on, which means turning the upper portion down and having
                      >>>> it ground for the high pressure seal, or start with a 4" shaft and turn
                      >>>> it down, leaving the center portion as the piston............ A LOT of
                      >>>> material to remove.
                      >>>>
                      >>>> The third option is to take a 1.5" shaft, and turn a groove into it
                      >>>> to accept a heavy snap ring or something of the sort, and simply pour
                      >>>> the ram right on the shaft. This of course means designing the mold so
                      >>>> I can turn out a pocket in the aluminum ram to accept a pressure seal or
                      >>>> just a high pressure O-ring. No big deal.
                      >>>>
                      >>>>
                      >>>> Option3 appeals to me.............. any thoughts?
                      >>>>
                      >>>> * Now to the why of it. The first part, the press design is pretty
                      >>>> obvious, but the ram design may not be as obvious to some. Here are the
                      >>>> reasons.
                      >>>>
                      >>>> 1: Keeping the spacing between the support points constant as the
                      >>>> cylinder extends. That is to say that with an ordinary cylinder, as the
                      >>>> ram approaches the end bushing any play is magnified. If you have a
                      >>>> couple thousandths of an inch at the top of the stroke, there will be
                      >>>> quite a bit by the time it is extended.
                      >>>>
                      >>>> 2: Impact......... I want a press where I can have an impact weight on
                      >>>> top....... lifted by air and dropped, and transmit that impact all the
                      >>>> way down through the ram. With impact, you can move something at 10
                      >>>> tons that would otherwise take the full 50 tons....... and not break it.
                      >>>>
                      >>>>
                      >>>> I would draw up a sketch, but I'm not much of a draftsman........ I
                      >>>> know what I want, and have a very clear picture in my head of
                      >>>> it............ enough to build it. I tend to do things that way.
                      >>>>
                      >>>>
                      >>>> Howard
                      >>>>
                      >>>
                      >>>
                      >>> ------------------------------------
                      >>>
                      >>> For discussion of Metal Casting and related issues
                      >>> this list does not accept attachments.
                      >>>
                      >>> Files area and list services are at:
                      >>> http://groups.yahoo.com/group/hobbicast
                      >>>
                      >>> For additional files and photos and off topic discussions
                      >>> check out these two affiliated sites:
                      >>> http://groups.yahoo.com/group/sandcrabs
                      >>> http://groups.yahoo.com/group/Hobbicast1
                      >>>
                      >>> Please visit our sponsor: Budget Casting Supply
                      >>> http://budgetcastingsupply.com/
                      >>>
                      >>> List Owner:
                      >>> owly@...
                      >>>
                      >>> Yahoo! Groups Links
                      >>>
                      >>>
                      >>>
                      >>>
                      >
                      >
                      >
                      > ------------------------------------
                      >
                      > For discussion of Metal Casting and related issues
                      > this list does not accept attachments.
                      >
                      > Files area and list services are at:
                      > http://groups.yahoo.com/group/hobbicast
                      >
                      > For additional files and photos and off topic discussions
                      > check out these two affiliated sites:
                      > http://groups.yahoo.com/group/sandcrabs
                      > http://groups.yahoo.com/group/Hobbicast1
                      >
                      > Please visit our sponsor: Budget Casting Supply
                      > http://budgetcastingsupply.com/
                      >
                      > List Owner:
                      > owly@...
                      >
                      > Yahoo! Groups Links
                      >
                      >
                      >
                      >
                    • Steven DePhillips
                      Here is a company that sells hydraulic cylinders and stuff at reasonable prices they also have surplus cylinders at even less.  I use them for a lot of my
                      Message 10 of 11 , Jan 25 7:10 AM
                        Here is a company that sells hydraulic cylinders and stuff at reasonable prices they also have surplus cylinders at even less.  I use them for a lot of my projects  http://www.baileynet.com/%c2%a0  They are in Tennessee  so i don't know ho much the shipping to you would be.  I live in Georgia so its not too bad.


                        ________________________________
                        From: StoneTool <owly@...>
                        To: hobbicast@yahoogroups.com
                        Sent: Thursday, January 24, 2013 10:51 PM
                        Subject: Re: [hobbicast] Re: press project


                         
                        I have a 50 ton ram with 8" stroke that has a solid brass ram &
                        piston............

                        Howard

                        On 01/24/2013 03:23 PM, redlupmi2 wrote:
                        > Glad to know you have experience with 50 ton presses. Some pay a high price for the experience.
                        >
                        > A local hydraulic cylinder builder takes a steel piston and brazes a layer of brass or welds a layer of silicon bronze to the OD of some of their pistons then machines to finish size.
                        >
                        > R.T. :D
                        >
                        > --- In hobbicast@yahoogroups.com, StoneTool wrote:
                        >> RT:
                        >> Thanks for the share............
                        >>
                        >> I work with 50 ton stuff all the time
                        >>
                        >> I agree that an aluminum piston will not transmit 50 T to a
                        >> 1.5" rod without deforming unless there is steel to spread the force out
                        >> wider. I like an Aluminum piston because of wear. I've seen too many
                        >> steel pistons gall cylinders when the wear bands don't quite do the
                        >> job. In addition seals for that kind of pressure must run at VERY close
                        >> tolerance. I don't like steel on steel when tolerances are very
                        >> close. Cast iron on steel works well, as does brass or aluminum.
                        >> I share your concerns about things blowing out of presses to the
                        >> extent that I once built a press based on a 1" thick steel table with
                        >> various openings, and the press portion moved up and down so your
                        >> working height was always the table top. The idea was to weld support
                        >> structures right to the table for pressing so everything was rigid.
                        >> It's a good machine and still in service. A 12" centrally located round
                        >> hole with a flange beneath it for reinforcement is the primary work
                        >> area, and press blocks of 1" plate are used to bridge the hole. It also
                        >> has a slot 8" wide and a number of other holes, and the cylinder can be
                        >> located at virtually any point on the surface. It uses a 50 ton
                        >> Owatanna porta power cylinder and electric pump. A rather unique and
                        >> elegant system that cost a lot of money by the time I was done...... I
                        >> don't own it and couldn't afford to build one like it for my own use.
                        >> Threaded rods across between the table sections may be needed on
                        >> the press I'm contemplating to maintain their relationship, though I'm
                        >> looking at other and more convenient means of securing them. Top
                        >> clamping alone is probably not enough. I've examined a lot of
                        >> different ways of doing things from top and bottom eccentric clamping to
                        >> hydraulic clamping with press pressure, to half nuts to other positive
                        >> dogging methods. I haven't nailed down a final design yet.
                        >>
                        >>
                        >> Howard
                        >>
                        >> On 01/23/2013 05:46 PM, redlupmi2 wrote:
                        >>> I'll share my experience.
                        >>>
                        >>> I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.
                        >>>
                        >>> My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.
                        >>>
                        >>> The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.
                        >>>
                        >>> Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.
                        >>>
                        >>> 4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.
                        >>>
                        >>> As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.
                        >>>
                        >>> Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.
                        >>>
                        >>> If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.
                        >>>
                        >>> Plan carefully, and work safely.
                        >>>
                        >>> R.T. :D
                        >>>
                        >>> --- In hobbicast@yahoogroups.com, StoneTool wrote:
                        >>>> I've been contemplating a shop press project that is rather unique.
                        >>>> The press consists of a set of legs on the floor to support it, and a
                        >>>> vertical post, with two parallel channels extending outward toward you,
                        >>>> and fairly high up. Two frames consisting of a top channel, a pair of
                        >>>> vertical square tubes, and a bottom tube hang from the two horizontal
                        >>>> channels that extend from the main post. Each of these frames is half
                        >>>> of the press frame, and has a channel table that can be raised or
                        >>>> lowered to the correct height. Because these frames are independent
                        >>>> and free floating, they can be slid to any spacing or angle desired.
                        >>>> Clamping bars above the top channels of these frames clamp them firmly
                        >>>> down to the two channels they hang from so they do not move once
                        >>>> placed. The two channels these frames hang from have the press cylinder
                        >>>> attached between them in a fixed location (center).
                        >>>>
                        >>>> Now that the above is clear as mud ;-)........... on to the
                        >>>> casting portion of the project:
                        >>>>
                        >>>> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                        >>>> is quite expensive and not locally available. I propose to use
                        >>>> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                        >>>> diameter ordinary pipe, say 6", and pour the intervening space full of
                        >>>> aluminum
                        >>>>
                        >>>>
                        >>>> 2: This cylinder will have a ram that passes completely through both
                        >>>> ends, with the piston in the middle or thereabouts. The problem here
                        >>>> is that I need to attach a piston capable of transmitting 50 tons to the
                        >>>> ram. That means either I must use a stepped shaft so the piston has a
                        >>>> ledge to press on, which means turning the upper portion down and having
                        >>>> it ground for the high pressure seal, or start with a 4" shaft and turn
                        >>>> it down, leaving the center portion as the piston............ A LOT of
                        >>>> material to remove.
                        >>>>
                        >>>> The third option is to take a 1.5" shaft, and turn a groove into it
                        >>>> to accept a heavy snap ring or something of the sort, and simply pour
                        >>>> the ram right on the shaft. This of course means designing the mold so
                        >>>> I can turn out a pocket in the aluminum ram to accept a pressure seal or
                        >>>> just a high pressure O-ring. No big deal.
                        >>>>
                        >>>>
                        >>>> Option3 appeals to me.............. any thoughts?
                        >>>>
                        >>>> * Now to the why of it. The first part, the press design is pretty
                        >>>> obvious, but the ram design may not be as obvious to some. Here are the
                        >>>> reasons.
                        >>>>
                        >>>> 1: Keeping the spacing between the support points constant as the
                        >>>> cylinder extends. That is to say that with an ordinary cylinder, as the
                        >>>> ram approaches the end bushing any play is magnified. If you have a
                        >>>> couple thousandths of an inch at the top of the stroke, there will be
                        >>>> quite a bit by the time it is extended.
                        >>>>
                        >>>> 2: Impact......... I want a press where I can have an impact weight on
                        >>>> top....... lifted by air and dropped, and transmit that impact all the
                        >>>> way down through the ram. With impact, you can move something at 10
                        >>>> tons that would otherwise take the full 50 tons....... and not break it.
                        >>>>
                        >>>>
                        >>>> I would draw up a sketch, but I'm not much of a draftsman........ I
                        >>>> know what I want, and have a very clear picture in my head of
                        >>>> it............ enough to build it. I tend to do things that way.
                        >>>>
                        >>>>
                        >>>> Howard
                        >>>>
                        >>>
                        >>>
                        >>> ------------------------------------
                        >>>
                        >>> For discussion of Metal Casting and related issues
                        >>> this list does not accept attachments.
                        >>>
                        >>> Files area and list services are at:
                        >>> http://groups.yahoo.com/group/hobbicast
                        >>>
                        >>> For additional files and photos and off topic discussions
                        >>> check out these two affiliated sites:
                        >>> http://groups.yahoo.com/group/sandcrabs
                        >>> http://groups.yahoo.com/group/Hobbicast1
                        >>>
                        >>> Please visit our sponsor: Budget Casting Supply
                        >>> http://budgetcastingsupply.com/
                        >>>
                        >>> List Owner:
                        >>> owly@...
                        >>>
                        >>> Yahoo! Groups Links
                        >>>
                        >>>
                        >>>
                        >>>
                        >
                        >
                        >
                        > ------------------------------------
                        >
                        > For discussion of Metal Casting and related issues
                        > this list does not accept attachments.
                        >
                        > Files area and list services are at:
                        > http://groups.yahoo.com/group/hobbicast
                        >
                        > For additional files and photos and off topic discussions
                        > check out these two affiliated sites:
                        > http://groups.yahoo.com/group/sandcrabs
                        > http://groups.yahoo.com/group/Hobbicast1
                        >
                        > Please visit our sponsor: Budget Casting Supply
                        > http://budgetcastingsupply.com/
                        >
                        > List Owner:
                        > owly@...
                        >
                        > Yahoo! Groups Links
                        >
                        >
                        >
                        >




                        [Non-text portions of this message have been removed]
                      • StoneTool
                        Steven: I do business with Bailey all the time........ My cylinder design is significantly different from anything I can readily buy off the shelf. The ram
                        Message 11 of 11 , Jan 25 9:31 AM
                          Steven:
                          I do business with Bailey all the time........

                          My cylinder design is significantly different from anything I can
                          readily buy off the shelf. The ram passing completely through the
                          cylinder is an important feature for several reasons. I want to be
                          able to impact the press by jarring the top of the ram, and I also want
                          the stability of having two bushings that remain at the same spacing,
                          rather than the single lower bushing and the ram, which approach each
                          other as the ram extends. That reducing spacing as the ram extends
                          results in more side play as you work further extended. The 10000 psi
                          pressure range matters in terms of size. It would take an 8" cylinder
                          to accomplish the same thing on "conventional pressures". I can get 4"
                          x 4.75" material at the local hydraulic shop where I have an account and
                          get fairly decent prices.


                          Howard



                          On 01/25/2013 08:10 AM, Steven DePhillips wrote:
                          > Here is a company that sells hydraulic cylinders and stuff at reasonable prices they also have surplus cylinders at even less. I use them for a lot of my projects http://www.baileynet.com/ They are in Tennessee so i don't know ho much the shipping to you would be. I live in Georgia so its not too bad.
                          >
                          >
                          > ________________________________
                          > From: StoneTool<owly@...>
                          > To: hobbicast@yahoogroups.com
                          > Sent: Thursday, January 24, 2013 10:51 PM
                          > Subject: Re: [hobbicast] Re: press project
                          >
                          >
                          >
                          > I have a 50 ton ram with 8" stroke that has a solid brass ram&
                          > piston............
                          >
                          > Howard
                          >
                          > On 01/24/2013 03:23 PM, redlupmi2 wrote:
                          >> Glad to know you have experience with 50 ton presses. Some pay a high price for the experience.
                          >>
                          >> A local hydraulic cylinder builder takes a steel piston and brazes a layer of brass or welds a layer of silicon bronze to the OD of some of their pistons then machines to finish size.
                          >>
                          >> R.T. :D
                          >>
                          >> --- In hobbicast@yahoogroups.com, StoneTool wrote:
                          >>> RT:
                          >>> Thanks for the share............
                          >>>
                          >>> I work with 50 ton stuff all the time
                          >>>
                          >>> I agree that an aluminum piston will not transmit 50 T to a
                          >>> 1.5" rod without deforming unless there is steel to spread the force out
                          >>> wider. I like an Aluminum piston because of wear. I've seen too many
                          >>> steel pistons gall cylinders when the wear bands don't quite do the
                          >>> job. In addition seals for that kind of pressure must run at VERY close
                          >>> tolerance. I don't like steel on steel when tolerances are very
                          >>> close. Cast iron on steel works well, as does brass or aluminum.
                          >>> I share your concerns about things blowing out of presses to the
                          >>> extent that I once built a press based on a 1" thick steel table with
                          >>> various openings, and the press portion moved up and down so your
                          >>> working height was always the table top. The idea was to weld support
                          >>> structures right to the table for pressing so everything was rigid.
                          >>> It's a good machine and still in service. A 12" centrally located round
                          >>> hole with a flange beneath it for reinforcement is the primary work
                          >>> area, and press blocks of 1" plate are used to bridge the hole. It also
                          >>> has a slot 8" wide and a number of other holes, and the cylinder can be
                          >>> located at virtually any point on the surface. It uses a 50 ton
                          >>> Owatanna porta power cylinder and electric pump. A rather unique and
                          >>> elegant system that cost a lot of money by the time I was done...... I
                          >>> don't own it and couldn't afford to build one like it for my own use.
                          >>> Threaded rods across between the table sections may be needed on
                          >>> the press I'm contemplating to maintain their relationship, though I'm
                          >>> looking at other and more convenient means of securing them. Top
                          >>> clamping alone is probably not enough. I've examined a lot of
                          >>> different ways of doing things from top and bottom eccentric clamping to
                          >>> hydraulic clamping with press pressure, to half nuts to other positive
                          >>> dogging methods. I haven't nailed down a final design yet.
                          >>>
                          >>>
                          >>> Howard
                          >>>
                          >>> On 01/23/2013 05:46 PM, redlupmi2 wrote:
                          >>>> I'll share my experience.
                          >>>>
                          >>>> I don't think an aluminum piston will transmit that much pressure to a 1-1/2" steel rod, without deforming. Besides the columnar strength required due to length.
                          >>>>
                          >>>> My 25T Dake has deformed the end of the 1-1/4" diameter screw many times. And has swelled the ends of CRS 1" dia. push pins to hour glass shape. I was hiding behind the upright as best I could, to avoid possible shrapnel.
                          >>>>
                          >>>> The 25T Dake has a 3-7/8" dia. bore and 2-1/2" rod, with 1-1/2" adjusting screw with currently 1-1/4" end.
                          >>>>
                          >>>> Have a 150T Dake 8" dia. bore, also. It is scary when using it, as everything has to be secure, and perpendicular. Any miss alignment and those big blocks travel a loooooooooog way when anything slips.
                          >>>>
                          >>>> 4"id x 5"OD tubing is readily available from my usual source Bailey Sales Knoxville, TN. (They sell components too) But looks like 1-1/4" wall is used by the ones using 10k psi and required to stand behind or beside their products.
                          >>>>
                          >>>> As for securing the piston to the rod for a double ended cylinder, I would have an interference fit (.001/inch) between the piston and rod, with a three piece ring to slip into the appropriate groove machined in the rod, and secured by a counterbore in the piston. The three piece ring has to withstand the shearing force of the pressure applied to the piston.
                          >>>>
                          >>>> Heat piston, quickly slip on rod, while securing three piece ring. I've worked on lower pressure double end cylinders the piston was only secured by the interference fit. And these cylinders were required to push and pull, where your design only requires high pressure one direction.
                          >>>>
                          >>>> If in doubt, could install a spiral lock retaining ring above the piston for peace of mind.
                          >>>>
                          >>>> Plan carefully, and work safely.
                          >>>>
                          >>>> R.T. :D
                          >>>>
                          >>>> --- In hobbicast@yahoogroups.com, StoneTool wrote:
                          >>>>> I've been contemplating a shop press project that is rather unique.
                          >>>>> The press consists of a set of legs on the floor to support it, and a
                          >>>>> vertical post, with two parallel channels extending outward toward you,
                          >>>>> and fairly high up. Two frames consisting of a top channel, a pair of
                          >>>>> vertical square tubes, and a bottom tube hang from the two horizontal
                          >>>>> channels that extend from the main post. Each of these frames is half
                          >>>>> of the press frame, and has a channel table that can be raised or
                          >>>>> lowered to the correct height. Because these frames are independent
                          >>>>> and free floating, they can be slid to any spacing or angle desired.
                          >>>>> Clamping bars above the top channels of these frames clamp them firmly
                          >>>>> down to the two channels they hang from so they do not move once
                          >>>>> placed. The two channels these frames hang from have the press cylinder
                          >>>>> attached between them in a fixed location (center).
                          >>>>>
                          >>>>> Now that the above is clear as mud ;-)........... on to the
                          >>>>> casting portion of the project:
                          >>>>>
                          >>>>> 1: The material required to build a 4" cylinder capable of 10,000 PSI
                          >>>>> is quite expensive and not locally available. I propose to use
                          >>>>> ordinary 3/8" wall 4" honed tubing, place it inside considerably larger
                          >>>>> diameter ordinary pipe, say 6", and pour the intervening space full of
                          >>>>> aluminum
                          >>>>>
                          >>>>>
                          >>>>> 2: This cylinder will have a ram that passes completely through both
                          >>>>> ends, with the piston in the middle or thereabouts. The problem here
                          >>>>> is that I need to attach a piston capable of transmitting 50 tons to the
                          >>>>> ram. That means either I must use a stepped shaft so the piston has a
                          >>>>> ledge to press on, which means turning the upper portion down and having
                          >>>>> it ground for the high pressure seal, or start with a 4" shaft and turn
                          >>>>> it down, leaving the center portion as the piston............ A LOT of
                          >>>>> material to remove.
                          >>>>>
                          >>>>> The third option is to take a 1.5" shaft, and turn a groove into it
                          >>>>> to accept a heavy snap ring or something of the sort, and simply pour
                          >>>>> the ram right on the shaft. This of course means designing the mold so
                          >>>>> I can turn out a pocket in the aluminum ram to accept a pressure seal or
                          >>>>> just a high pressure O-ring. No big deal.
                          >>>>>
                          >>>>>
                          >>>>> Option3 appeals to me.............. any thoughts?
                          >>>>>
                          >>>>> * Now to the why of it. The first part, the press design is pretty
                          >>>>> obvious, but the ram design may not be as obvious to some. Here are the
                          >>>>> reasons.
                          >>>>>
                          >>>>> 1: Keeping the spacing between the support points constant as the
                          >>>>> cylinder extends. That is to say that with an ordinary cylinder, as the
                          >>>>> ram approaches the end bushing any play is magnified. If you have a
                          >>>>> couple thousandths of an inch at the top of the stroke, there will be
                          >>>>> quite a bit by the time it is extended.
                          >>>>>
                          >>>>> 2: Impact......... I want a press where I can have an impact weight on
                          >>>>> top....... lifted by air and dropped, and transmit that impact all the
                          >>>>> way down through the ram. With impact, you can move something at 10
                          >>>>> tons that would otherwise take the full 50 tons....... and not break it.
                          >>>>>
                          >>>>>
                          >>>>> I would draw up a sketch, but I'm not much of a draftsman........ I
                          >>>>> know what I want, and have a very clear picture in my head of
                          >>>>> it............ enough to build it. I tend to do things that way.
                          >>>>>
                          >>>>>
                          >>>>> Howard
                          >>>>>
                          >>>>
                          >>>> ------------------------------------
                          >>>>
                          >>>> For discussion of Metal Casting and related issues
                          >>>> this list does not accept attachments.
                          >>>>
                          >>>> Files area and list services are at:
                          >>>> http://groups.yahoo.com/group/hobbicast
                          >>>>
                          >>>> For additional files and photos and off topic discussions
                          >>>> check out these two affiliated sites:
                          >>>> http://groups.yahoo.com/group/sandcrabs
                          >>>> http://groups.yahoo.com/group/Hobbicast1
                          >>>>
                          >>>> Please visit our sponsor: Budget Casting Supply
                          >>>> http://budgetcastingsupply.com/
                          >>>>
                          >>>> List Owner:
                          >>>> owly@...
                          >>>>
                          >>>> Yahoo! Groups Links
                          >>>>
                          >>>>
                          >>>>
                          >>>>
                          >>
                          >>
                          >> ------------------------------------
                          >>
                          >> For discussion of Metal Casting and related issues
                          >> this list does not accept attachments.
                          >>
                          >> Files area and list services are at:
                          >> http://groups.yahoo.com/group/hobbicast
                          >>
                          >> For additional files and photos and off topic discussions
                          >> check out these two affiliated sites:
                          >> http://groups.yahoo.com/group/sandcrabs
                          >> http://groups.yahoo.com/group/Hobbicast1
                          >>
                          >> Please visit our sponsor: Budget Casting Supply
                          >> http://budgetcastingsupply.com/
                          >>
                          >> List Owner:
                          >> owly@...
                          >>
                          >> Yahoo! Groups Links
                          >>
                          >>
                          >>
                          >>
                          >
                          >
                          >
                          > [Non-text portions of this message have been removed]
                          >
                          >
                          >
                          > ------------------------------------
                          >
                          > For discussion of Metal Casting and related issues
                          > this list does not accept attachments.
                          >
                          > Files area and list services are at:
                          > http://groups.yahoo.com/group/hobbicast
                          >
                          > For additional files and photos and off topic discussions
                          > check out these two affiliated sites:
                          > http://groups.yahoo.com/group/sandcrabs
                          > http://groups.yahoo.com/group/Hobbicast1
                          >
                          > Please visit our sponsor: Budget Casting Supply
                          > http://budgetcastingsupply.com/
                          >
                          > List Owner:
                          > owly@...
                          >
                          > Yahoo! Groups Links
                          >
                          >
                          >
                          >
                        Your message has been successfully submitted and would be delivered to recipients shortly.