Re: New guy

Expand Messages
  • Lyle
    You won t need to stir them. They will completely dissolve without stirring and stirring disrupts the protective skim coat. LL
    Message 1 of 7 , Jan 31, 2009
    • 0 Attachment
      You won't need to stir them. They will completely dissolve without stirring and stirring
      disrupts the protective skim coat.
      LL

      --- In hobbicast@yahoogroups.com, "James Buchanan" <jambuch@...> wrote:
      >
      > Alloy 4 pounds of melted aluminum with 5.12 oz of short pieces of copper
      > wire. melt the aluminum and drop in the copper wire and stir until the
      > copper is dissolved.
      >
      > This works for cans and extruded aluminum.
      >
      > Jim
      >
      > __________________________________________________
      > James (Jim) Buchanan
      > Lexington, Kentucky
      > Climax Class B Locomotive Builder/Operator
      > GE 44 Ton Industrial Switcher Builder/Operator
      > Email: jambuch@...
      > Web Page: http://jambuch.home.insightbb.com
      >