    any of you cast stainless, what temp required pat
    Message 1 of 2 , Sep 6, 2005
    • 0 Attachment
      any of you cast stainless, what temp required

      pat
    • Rick Rowlands
      We pour stainless at 2900 F to 2950 F. Anything less and you risk cold laps and ladle freezups. Rick ... From: pat176_6 To:
      Message 2 of 2 , Sep 6, 2005
      • 0 Attachment
        We pour stainless at 2900 F to 2950 F. Anything less and you risk cold laps
        and ladle freezups.

        Rick
        ----- Original Message -----
        From: "pat176_6" <goldenvirginia@...>
        To: <hobbicast@yahoogroups.com>
        Sent: Tuesday, September 06, 2005 3:42 PM
        Subject: [hobbicast] stainless


        > any of you cast stainless, what temp required
        >
        > pat
        >
        >
        >
        >
        >
        > For discussion of Metal Casting and related issues
        > this list does not accept attachments.
        >
        > Files area and list services are at:
        > http://groups.yahoo.com/group/hobbicast
        >
        > For additional files and photos and off topic discussions
        > check out these two affiliated sites:
        > http://groups.yahoo.com/group/sandcrabs
        > http://groups.yahoo.com/group/Hobbicast1
        >
        > Please visit our sponsor: Budget Casting Supply
        > http://budgetcastingsupply.com/
        >
        > List Owner:
        > owly@...
        >
        >
        > Yahoo! Groups Links
        >
        >
        >
        >
        >
        >
      Your message has been successfully submitted and would be delivered to recipients shortly.