    I was told last night by a bullet caster that the alloy has been changed in the US. He didn t know what it was, but it melts at a higher temperature. Any
    Message 1 of 8 , Mar 3, 2003
      I was told last night by a bullet caster that the alloy has been changed in
      the US. He didn't know what it was, but it melts at a higher temperature.
      Any clues as to what this might be? Dan P
      ----- Original Message -----
      From: "john grant" <grantjoh@...>
      To: <hobbicast@yahoogroups.com>
      Sent: Sunday, March 02, 2003 3:50 PM
      Subject: Re: [hobbicast] lead/antimony


      > There may be some antimony to harden them but I can see no reason to use a
      more expensive metal when lead will do.
      >
      > "Brent " wrote:
      >
      > > Are automotive wheel wieghts made from lead as everyone thinks, or
      > > antimony, which I was told by someone?
      > > Brent
      > >
      > > This list is for discussion of metal casting
      > > and does not accept attachments. For off topic discussion and to share
      photos and stuff: join Sandcrabs by sending a blank message to:
      sandcrabs-subscribe@yahoogroups.com
      > > http://groups.yahoo.com/group/sandcrabs
      > > or join the Coffee Lounge group (by approval)
      > > http://groups.yahoo.com/group/Hobbicast_coffee_lounge/
      > >
      > > Please visit our sponsor: Budget Casting Supply
      > > http://budgetcastingsupply.com/
      > >
      > > Files area and list services are at:
      > > http://groups.yahoo.com/group/hobbicast
      > >
      > > To unsubscribe from this group, send an email to:
      > > hobbicast-unsubscribe@yahoogroups.com
      > >
      > > For problems that cannot be otherwise solved contact the list owner by
      email:
      > > owly@...
      > >
      > >
      > >
      > > Your use of Yahoo! Groups is subject to
      http://docs.yahoo.com/info/terms/
      >
      >
      > This list is for discussion of metal casting
      > and does not accept attachments. For off topic discussion and to share
      photos and stuff: join Sandcrabs by sending a blank message to:
      sandcrabs-subscribe@yahoogroups.com
      > http://groups.yahoo.com/group/sandcrabs
      > or join the Coffee Lounge group (by approval)
      > http://groups.yahoo.com/group/Hobbicast_coffee_lounge/
      >
      > Please visit our sponsor: Budget Casting Supply
      > http://budgetcastingsupply.com/
      >
      > Files area and list services are at:
      > http://groups.yahoo.com/group/hobbicast
      >
      > To unsubscribe from this group, send an email to:
      > hobbicast-unsubscribe@yahoogroups.com
      >
      > For problems that cannot be otherwise solved contact the list owner by
      email:
      > owly@...
      >
      >
      >
      > Your use of Yahoo! Groups is subject to http://docs.yahoo.com/info/terms/
      >
      >
    • Tony Wells
      Try the Yahoo bullet casting group, perhaps they will be able to help you. It is CB-L@yahoogroups.com Here in the UK the alloy is 96%lead and 4% antimony
      Message 2 of 8 , Mar 3, 2003
        Try the Yahoo bullet casting group, perhaps they will be able to help you.
        It is CB-L@yahoogroups.com Here in the UK the alloy is 96%lead and 4%
        antimony (there is supposed to be a small amount of tin present, but usually
        gets lost in the re-cycling). Chatting to some of the American bullet
        casters there are various tales of wheelweight alloy running from 3% to 5%
        antimony. You could always cast something in it, then weight the casting in
        air and then suspended in water to calculate it's specific gravity and work
        backwards from that to find the ration of the antimony and the tin.

        Tony Wells.


        ----- Original Message -----
        From: "Daniel C. Postellon" <postello@...>
        To: <hobbicast@yahoogroups.com>
        Sent: Monday, March 03, 2003 12:07 PM
        Subject: Re: [hobbicast] lead/antimony


        > I was told last night by a bullet caster that the alloy has been changed
        in
        > the US. He didn't know what it was, but it melts at a higher temperature.
        > Any clues as to what this might be? Dan P
        > ----- Original Message -----
        > From: "john grant" <grantjoh@...>
        > To: <hobbicast@yahoogroups.com>
        > Sent: Sunday, March 02, 2003 3:50 PM
        > Subject: Re: [hobbicast] lead/antimony
        >
        >
        > > There may be some antimony to harden them but I can see no reason to use
        a
        > more expensive metal when lead will do.
        > >
        > > "Brent " wrote:
        > >
        > > > Are automotive wheel wieghts made from lead as everyone thinks, or
        > > > antimony, which I was told by someone?
        > > > Brent
        > > >