Loading ...
Sorry, an error occurred while loading the content.

8724Re: [hobbicast] TO: Dale Smith

Expand Messages
  • Dale Smith
    Dec 1, 2001
      Thanks Bill,

      Add me to the URL/Phone # request.

      I guess the thing that attracts me is rubbing cyber elbows with the H'wood
      special effects crowd. If I had life to live over, and everything would be
      perfect, I can't imagine a job more suited to my likes and loves as special
      effects. I cast my vote for John He to take up that line of work. Just
      think, he would have a large budget and get paid to do everything he is
      dreaming about right now.

      wdsmith

      ----- Original Message -----
      From: "Jack Fuselier" <gunsmith@...>
      To: <hobbicast@yahoogroups.com>
      Sent: Saturday, December 01, 2001 5:51 AM
      Subject: Re: [hobbicast] TO: Dale Smith


      > How about a url or phone number on that cementex supplier Jack F
      >
      > boyerw@... wrote:
      > >
      > > Hi Dale
      > > I Brush on 13 layers of latex. Every 4th layer is backed up with 1"
      > > strips of cheeze cloth. after the first coat, I thicken the latez
      > > with ceco powder so the latex will not run down the sides of the
      > > model. Like Lyle said you can expand the mold about 40% with naptha.
      > > I get ny laytex from cementex in NY for $28:00 gl and it goes a long
      > > way
      > > Bill Boyer
      >
      > =================