      I Brush on 13 layers of latex. Every 4th layer is backed up with 1"
      strips of cheeze cloth. after the first coat, I thicken the latez
      with ceco powder so the latex will not run down the sides of the
      model. Like Lyle said you can expand the mold about 40% with naptha.
      I get ny laytex from cementex in NY for $28:00 gl and it goes a long
      way
      Bill Boyer