42832Re: [hobbicast] new article: Laser Printing to Powder Coated Sheet Aluminum

Expand Messages
  • Rick Sparber
    Aug 18, 2013
      Howard,

      Many people use irons. I've never gotten consistent results with one. You need to be at about 250° F I believe.

      Rick


      On Aug 18, 2013, at 6:42 PM, StoneTool <owly@...> wrote:

      > Rick:
      > This is really interesting and useful........... I can see dozens
      > of applications. Thanks for posting that. I'm wondering if one could
      > use an ordinary iron to accomplish the transfer.
      >
      > Howard