42473Re: [hobbicast] ingate / outgate

Expand Messages
  • David Patterson
    Jan 5, 2013
      Nelson no need to say sorry. Just pointing out where the picture came from. I thought is was somewhat funny that the picture you showed was the same as the one I happen to look at the day before while scanning the the link. I did give a better example for casting plaques, that showed what I tried to explain below.  There are at least 3 things that can give you a bad casting, poorly made pattern, improperly maintained sand and improperly designed gating system.
       
      Some will start casting something and have problems, then guess at what the problem is. After a few castings they might have stumbled of something that works, without understanding what they did. The next casting that's similar they gate the same way and it doesn't work , so what happened? They don't know. I just point out the need to read, understand and try to apply what others have done, before you start casting. Does not have to be a college level study session, just a little research,on line or in books. If done this way your results will improve faster without so much trial and error. But I've always done this when starting a new endeavor.
       
      So have a great year and many good casting sessions,
       
      Dave Patterson
      odd_kins@...
      http://home.comcast.net/~oddkins/foundry_home.html

      --- On Sat, 1/5/13, Nelson Collar <nel2lar@...> wrote:


      From: Nelson Collar <nel2lar@...>
      Subject: Re: [hobbicast] ingate / outgate
      To: "hobbicast@yahoogroups.com" <hobbicast@yahoogroups.com>
      Date: Saturday, January 5, 2013, 7:46 AM



       



      Dave 
      Yes
      it is from the Navy book. It was just for to show how the C runner
      and nothing else. I do not understand what all the negativity is all
      about. I started in the late 90's and I feel I can make anything I
      want to. If I can help some one out that what it is about? If you
      have a better way, tell him how you would do it. That is what Sage
      needs so give it to him. Sage try and try again, you will find
      something that will work, just do not get disgusted with the not
      complete fills.

      Dave if I ruffled your feathers, I'm sorry. Good day

      Nelson Collar 
         

      ________________________________
      From: David Patterson odd_kins@...>
      To: hobbicast@yahoogroups.com
      Sent: Friday, January 4, 2013 10:15 PM
      Subject: Re: [hobbicast] ingate / outgate


       
      Nelson that is a picture out of the manual Sage sent you. It's an impeller housing found of page 77 figure 89. The large void is not a riser it's a reservoir used to trap any imputities in the metal before entering the runner. If casting a round plaque one to two ingates will work one to two on each side of the sprue. Same would be true for a rectangular plaque, the runner would be more squared off with the largest radius you can put into the corners where the runner changes direction. tapering the runner or stepping runner thickness between each ingate. A riser is not needed when casting a plaque under 3/8" overall thickness. Understand I'm not a professional molder, I'm a patternmaker. When it comes to designing a gating system you always call in the journeyman molder, he knows best. I am only repeating what has be learned from these molders during my time spent in the pattern shop.

      Dave Patterson
      odd_kins@...
      http://home.comcast.net/~oddkins/foundry_home.html

      --- On Fri, 1/4/13, Nelson Collar nel2lar@...> wrote:

      From: Nelson Collar nel2lar@...>
      Subject: Re: [hobbicast] ingate / outgate
      To: "hobbicast@yahoogroups.comhobbicast@yahoogroups.com>
      Date: Friday, January 4, 2013, 4:47 PM

       

      Sage
      I knew in my files I had a pic that would demonstrate how to mold your plaque. 
      I told you to use a C runner, here is a pic with the C runner. If you look there are three spots the metal enters the plaque. And look at the pic where it looks like a coma. The small end is the sprue and the large portion is the riser, then it goes into the C to get your mold. It seems to be a long way to get it but I feel it will solve your problem. Blow the pic up and study it. The part they made was different than yours, but it should work. Look at how the metal goes through the runner and enters the mold at 10, 1 o'clock and about 6:30. The pis is loaded in the photos section under Nelson Collar this should get you there. http://groups.yahoo.com/group/hobbicast/photos/album/1125913416/pic/237319085/view?picmode=&mode=tn&order=ordinal&start=1&count=20&dir=asc
      Good luck
      Nelson Collar 

      ________________________________
      From: Nelson Collar nel2lar@...>
      To: "hobbicast@yahoogroups.comhobbicast@yahoogroups.com>
      Sent: Friday, January 4, 2013 5:31 PM
      Subject: Re: [hobbicast] ingate / outgate

       
      Sage
      As I responded earlier, when casting thin it better done in brass. But it can be done, it just takes time to figure out what works. What I would try is to put a "C" shape runner placing your plaque in the middle. Run a lot of holes so the mold gases can have somewhere to go. Make sure the mold is face down, that way you will get a better looking plaque. The thing is not to give up and if it takes 10 times, remember you are having fun with what you do. Or you would not do it.
      Nelson Collar

      ________________________________
      From: Sage McGirk freeflysage@...>
      To: hobbicast@yahoogroups.com
      Sent: Friday, January 4, 2013 12:41 PM
      Subject: Re: [hobbicast] ingate / outgate

      i'm not an amateur or an expert.. I've done about 50 lost foam castings,
      and finally seeing the light with wood objects.  I'm really just having
      issues with thin objects, and haven't done a round/circular object before.
      I've seen some large foam circular objects and they angle 4 sprues into a
      single point from my research.  I have no problem with trial and error but
      dont like wasting my time if I can lean on the community for advice....

      FWIW

      /sm

      On Fri, Jan 4, 2013 at 12:32 PM, Nelson Collar nel2lar@...> wrote:

      > **
      >
      >
      > Well
      > I guess I missed something. If you read it all, When we start trying
      > to do things in the home shop perfection is not necessary. The sprue
      > does not require all the technical data. I use the same sprue for all
      > of my pours. Sometimes I use a riser, and I put the riser before the
      > cavity that way is ant bad metal will rise up the riser instead of
      > the pattern, and also helps preventing the part to be full with no
      > voids or over shrinkage. Cast can be a very rewarding skill, but if
      > we get all bogged up in things that have no call for at all. Like I
      > said about my South Bend, it has some areas that needed cosmetic
      > work. If the casting is made rigid it will withstand a lick-en and
      > still hold up. For the first timer, read and read some more, but do
      > not approach like it has to be perfect. The best way to get good at
      > anything we must start some where. If the simple guidelines are
      > followed it should yield good and workable parts. The more we
      > practice the more experience we will gain and hopefully the better we
      > will get as we hon our skills. I know how to cast and the advice to others
      > is to jump in and do something. Read and follow what others have done.
      > Good-Day
      >
      > Nelson Collar
      >
      > ________________________________
      > From: David Patterson odd_kins@...>
      > To: hobbicast@yahoogroups.com
      > Sent: Thursday, January 3, 2013 7:06 PM
      >
      > Subject: Re: [hobbicast] ingate / outgate
      >
      >
      >
      >
      > I did keep it simple. Someone asked a question and the last thing I would
      > tell anyone is to start casting so you can make chips. Making a working
      > casting and making a good casting are two different things. I would like to
      > see people making good, solid and clean looking castings. Following a few
      > simple rules for gating will make your chances better. If you want a
      > working casting, by all means, guess at the gating, guess if it needs
      > risers or not. And when your done if it's not perfect, Bondo the voids
      > and paint the casting to hide the defects. I would just as soon not but
      > that is just me. And yes I do analyze my pours, if I don't get a good
      > casting I will cut it up to find out what went wrong. Then try to correct
      > the problem.
      >
      > Dave Patterson
      > odd_kins@...
      > http://home.comcast.net/~oddkins/foundry_home.html
      >
      > --- On Thu, 1/3/13, Nelson Collar nel2lar@...> wrote:
      >
      > From: Nelson Collar nel2lar@...>
      > Subject: Re: [hobbicast] ingate / outgate
      > To: "hobbicast@yahoogroups.comhobbicast@yahoogroups.com>
      > Date: Thursday, January 3, 2013, 11:21 AM
      >
      >
      >
      >
      > Why are you being so technical about it. You are doing something that only
      > care needs be heeded. As far as pour rates and all that info has no bearing
      > to us, just that the cavity fills and is useable. Its bad enough if you try
      > to make something bigger than directed, because there are things you
      > overlook until you are done and you need to make changes. I know I made the
      > shaper larger to 8 inches and overlooked a few things. Be realistic and
      > start doing something to make chips. And yes all that high tech stuff is
      > not needed. Next thing you will start to analyze
      > your metal pours. Which is impossible because we can not get the
      > equipment to change anything before pouring. If you never heard the
      > K.I.S.S. explained well, Keep It Simple S****d. Make some castings so
      > you can make some chips.
      >
      > Nelson Collar
      >
      > ________________________________
      > From: David Patterson odd_kins@...>
      > To: hobbicast@yahoogroups.com
      > Sent: Wednesday, January 2, 2013 3:49 PM
      > Subject: Re: [hobbicast] ingate / outgate
      >
      >
      > You need to calulate the amount of time you need to fill the mold cavity.
      > Then starting from the ingates calulate the size needed to fill the cavity
      > in that time. Shape and number of the ingates will be dictated by the shape
      > of the casting. The cross sectional area of the runner/runners will be
      > equal to the sectional area of the ingate/ingates. The sectional area of
      > the sprue(smallest diameter) will be 1/4 the area of the runner. But this
      > is just a starting point, you adjust from here until you get a good
      > casting. Don't forget to cut a pouring basin into the cope, about 3 times
      > the diameter of the sprue. This is a 1-4-4 ratio used in non ferrous
      > foundrys, 1 is the sectional area of the sprue, 4 sectional area of all
      > runners and 4 sectional area of all ingates. Beyoud this trial and error
      > until you find what works.
      >
      > The idea is to keep the sprue full during the pour, keeping turbulance to
      > a minimum.
      > Thin casting that don't require risers, vent, a lot if unsure. Risers will
      > act as vents in larger casting.
      >
      > The only reason to have a second sprue(outgate) would be if you have 2
      > people pouring at the same time.
      >
      > Dave Patterson
      > odd_kins@...
      > http://home.comcast.net/~oddkins/foundry_home.html
      >
      > --- On Wed, 1/2/13, Sage McGirk freeflysage@...> wrote:
      >
      > From: Sage McGirk freeflysage@...>
      > Subject: [hobbicast] ingate / outgate
      > To: hobbicast@yahoogroups.com
      > Date: Wednesday, January 2, 2013, 11:09 AM
      >
      >
      >
      > Happy new year everyone! I've been hobbicasting for about 6/7 months
      > now, and I'm looking for any sort of rule of thumb for the size of the
      > ingate/outgate holes. I'm starting to cast some bigger objects (>
      > 3-4") that tend to be fairly thin. I've learned to POUR faster to
      > ensure nothing cools prematurely but find some objects still dont
      > quite finish. I'm guessing larger ingates are the trick. I'm also
      > about to embark on some gear shaped objects, and wondering how ,if
      > needed, to do multiple sprue holes as I've seen with lost foam, but
      > will be using wood as objects now. Any advice, video's, pictures
      > would be appreciated
      >
      > Thanks
      >
      > /sm
      >
      > [Non-text portions of this message have been removed]
      >
      > [Non-text portions of this message have been removed]
      >
      > [Non-text portions of this message have been removed]
      >
      > [Non-text portions of this message have been removed]
      >

      >

      [Non-text portions of this message have been removed]

      ------------------------------------

      For discussion of Metal Casting and related issues
      this list does not accept attachments. 

      Files area and list services are at:
          http://groups.yahoo.com/group/hobbicast

      For additional files and photos and off topic discussions
      check out these two affiliated sites:
          http://groups.yahoo.com/group/sandcrabs
          http://groups.yahoo.com/group/Hobbicast1

      Please visit our sponsor: Budget Casting Supply
      http://budgetcastingsupply.com/

      List Owner:
      owly@...

      Yahoo! Groups Links

      [Non-text portions of this message have been removed]

      [Non-text portions of this message have been removed]

      [Non-text portions of this message have been removed]

      [Non-text portions of this message have been removed]








      [Non-text portions of this message have been removed]
    • Show all 30 messages in this topic