  • Joseph Feldmann
    Jan 5, 2013
      Hey there, Folks-
        I'mfar less experienced than most of you, so take my comment with that in mind, but: I've found that round-shaped runners create less turbulence filling the mold than squared-off ones. Just my 2-cents-worth.

      Yvan Wolvesbane
      Pacifist ...with occasional lapses.


      >________________________________
      >From: Nelson Collar <nel2lar@...>
      >To: "hobbicast@yahoogroups.com" <hobbicast@yahoogroups.com>
      >Sent: Saturday, January 5, 2013 12:44 PM
      >Subject: Re: [hobbicast] ingate / outgate
      >

      >2.15 has a real nice curved runner. There is no set rule how they run just that the metal flows and does not freeze.
      >Nelson Collar
      >