      On Jan 6, 2012, at 6:18 PM, Carl wrote:

      > Ernie:That still looks like it would take a lot of time to get set up. I think the easiest way is to just hide a $20 thermocouple under a thin layer of refractory. I found a chart with pyrometric cones up to 3650 degrees F. I can get a 3000 degree one and see what the thermocouple is reading when the cone bends. That should get me in the ballpark without spending a lot of money. Thanks Carl

      I think you will find that your eyes will be far more sensitive to the color temperature than a thermocouple buried in refractory.


      Best,

      Jeshua Lacock