Expand Messages
  • Lyle
    May 3, 2006
      But's it's alot cheaper at other places. But it's still more
      expensive than greensand.
      LL

      --- In hobbicast@yahoogroups.com, "Rick Rowlands" <jrrowlands@...>
      wrote:
      >
      > That bentone is awfully expensive. I converted from nobake to
      greensand a
      > few months ago and so far I've only spent $10.00 on 50 bags of
      bentonite
      > from foundry auctions.
      >
      > Please tell me why the petrobond is better than greensand.
      Greensand works
      > great for me.
      >
      > Rick Rowlands
      > Tod Engine Works
      > Makers of Quality iron, steel, ductile iron
      > and nonferrous castings
      > 249 North Water Avenue
      > Sharon, PA 16146
      > 330-728-2799
      > Fax 330-759-1524
      > www.todengine.org/engineworks.html
      > ----- Original Message -----
      > From: "k2821" <powerhammer50@...>
      > To: <hobbicast@yahoogroups.com>
      > Sent: Friday, April 28, 2006 2:10 AM
      > Subject: [hobbicast] Bentone 34 - Petrobond I
      >
      >
      > >
      > >
      > > All,
      > >
      > > I have just added Petrobond Resin - Bentone 34 to my site as an
      item
      > > for sale. In either pound or bag lots. Shipping UPS from Denver
      CO.
      > > This is a white color, from Elementis. Paypal accepted on the
      site.
      > >
      > > http://www.copperstarways.com
      > >
      > > Happy casting.
      > > RKern
      > > CSW
      > >
      > >
      > >
      > >
      > >
      > >
      > >
      > > For discussion of Metal Casting and related issues
      > > this list does not accept attachments.
      > >
      > > Files area and list services are at:
      > > http://groups.yahoo.com/group/hobbicast
      > >
      > > For additional files and photos and off topic discussions
      > > check out these two affiliated sites:
      > > http://groups.yahoo.com/group/sandcrabs
      > > http://groups.yahoo.com/group/Hobbicast1
      > >
      > > Please visit our sponsor: Budget Casting Supply
      > > http://budgetcastingsupply.com/
      > >
      > > List Owner:
      > > owly@...
      > >
      > >
      > > Yahoo! Groups Links
      > >
      > >
      > >
      > >
      > >
      > >
      >
    • Show all 16 messages in this topic