      Like Clint says, you only need a Muller for initially mixing up your
      own batches, but you can still achieve this by hand anyway. I mixed
      up all my own KB in small batches by hand. I made up a very simple
      mixer that is attached to a drill which I use to condition/regel my
      KB when the Methonal eventually evaporates. Propylene Carbonate
      however doesnt dry out as quickly as methonal but I use this as its
      easier to source here in NZ (-:

      Edyn
      New Zealand



      --- In hobbicast@yahoogroups.com, "Daniel C Postellon" <postello@...>
      wrote:
      >
      > Do you absolutely need a muller to use petrobond.
      >
      > > "Rick Rowlands" wrote
      > >
      > > Please tell me why the petrobond is better than greensand.
      Greensand
      > > works great for me.
      > >
      > > I used greensand for a while before switching to PB, Like said
      you
      > > can Ram and pour a few days, weeks even months later!, It packs
      nice
      > > and tight, and alot cleaner to work with. The greenstrength of kb
      is
      > > far more superior to Greensand, Ive never had any drops with KB.
      At
      > > times when ramming moulds with big sections hanging in the cope
      Ive
      > > thought I should ram up some Gaggers and never and had no drops.
      Ive
      > > also found when pulling patterns the sand doesnt break at the
      edges
      > > like Greensand does, just some of the experiances Ive had.
      > >
      > > I love my KBond!!!!!!!!!!!!!!!! (- :
      > >
      > > Edyn, New Zealand
      > >
      > >
      > >
      > >> Rick Rowlands
      > >> Tod Engine Works
      > >> Makers of Quality iron, steel, ductile iron
      > >> and nonferrous castings
      > >> 249 North Water Avenue
      > >> Sharon, PA 16146
      > >> 330-728-2799
      > >> Fax 330-759-1524
      > >> www.todengine.org/engineworks.html
      > >> ----- Original Message -----
      > >> From: "k2821" <powerhammer50@>
      > >> To: <hobbicast@yahoogroups.com>
      > >> Sent: Friday, April 28, 2006 2:10 AM
      > >> Subject: [hobbicast] Bentone 34 - Petrobond I
      > >>
      > >>
      > >> >
      > >> >
      > >> > All,
      > >> >
      > >> > I have just added Petrobond Resin - Bentone 34 to my site as
      an
      > > item
      > >> > for sale. In either pound or bag lots. Shipping UPS from
      Denver
      > > CO.
      > >> > This is a white color, from Elementis. Paypal accepted on the
      > > site.
      > >> >
      > >> > http://www.copperstarways.com
      > >> >
      > >> > Happy casting.
      > >> > RKern
      > >> > CSW
      > >> >
      > >> >
      > >> >
      > >> >
      > >> >
      > >> >
      > >> >
      > >> > For discussion of Metal Casting and related issues
      > >> > this list does not accept attachments.
      > >> >
      > >> > Files area and list services are at:
      > >> > http://groups.yahoo.com/group/hobbicast
      > >> >
      > >> > For additional files and photos and off topic discussions
      > >> > check out these two affiliated sites:
      > >> > http://groups.yahoo.com/group/sandcrabs
      > >> > http://groups.yahoo.com/group/Hobbicast1
      > >> >
      > >> > Please visit our sponsor: Budget Casting Supply
      > >> > http://budgetcastingsupply.com/
      > >> >
      > >> > List Owner:
      > >> > owly@
      > >> >
      > >> >
      > >> > Yahoo! Groups Links
      > >> >
      > >> >
      > >> >
      > >> >
      > >> >
      > >> >
      > >>
      > >
      > >
      > >
      > >
      > >
      > >
      > >
      > > For discussion of Metal Casting and related issues
      > > this list does not accept attachments.
      > >
      > > Files area and list services are at:
      > > http://groups.yahoo.com/group/hobbicast
      > >
      > > For additional files and photos and off topic discussions
      > > check out these two affiliated sites:
      > > http://groups.yahoo.com/group/sandcrabs
      > > http://groups.yahoo.com/group/Hobbicast1
      > >
      > > Please visit our sponsor: Budget Casting Supply
      > > http://budgetcastingsupply.com/
      > >
      > > List Owner:
      > > owly@...
      > >
      > >
      > > Yahoo! Groups Links
      > >
      > >
      > >
      > >
      > >
      > >
      > >
      >
    • Show all 16 messages in this topic