      Do you absolutely need a muller to use petrobond.

      > "Rick Rowlands" wrote
      >
      > Please tell me why the petrobond is better than greensand. Greensand
      > works great for me.
      >
      > I used greensand for a while before switching to PB, Like said you
      > can Ram and pour a few days, weeks even months later!, It packs nice
      > and tight, and alot cleaner to work with. The greenstrength of kb is
      > far more superior to Greensand, Ive never had any drops with KB. At
      > times when ramming moulds with big sections hanging in the cope Ive
      > thought I should ram up some Gaggers and never and had no drops. Ive
      > also found when pulling patterns the sand doesnt break at the edges
      > like Greensand does, just some of the experiances Ive had.
      >
      > I love my KBond!!!!!!!!!!!!!!!! (- :
      >
      > Edyn, New Zealand
      >
      >
      >
      >> Rick Rowlands
      >> Tod Engine Works
      >> Makers of Quality iron, steel, ductile iron
      >> and nonferrous castings
      >> 249 North Water Avenue
      >> Sharon, PA 16146
      >> 330-728-2799
      >> Fax 330-759-1524
      >> www.todengine.org/engineworks.html
      >> ----- Original Message -----
      >> From: "k2821" <powerhammer50@...>
      >> To: <hobbicast@yahoogroups.com>
      >> Sent: Friday, April 28, 2006 2:10 AM
      >> Subject: [hobbicast] Bentone 34 - Petrobond I
      >>
      >>
      >> >
      >> >
      >> > All,
      >> >
      >> > I have just added Petrobond Resin - Bentone 34 to my site as an
      > item
      >> > for sale. In either pound or bag lots. Shipping UPS from Denver
      > CO.
      >> > This is a white color, from Elementis. Paypal accepted on the
      > site.
      >> >
      >> > http://www.copperstarways.com
      >> >
      >> > Happy casting.
      >> > RKern
      >> > CSW
      >> >
      >> >
      >> >
      >> >
      >> >
      >> >
      >> >
      >> > For discussion of Metal Casting and related issues
      >> > this list does not accept attachments.
      >> >
      >> > Files area and list services are at:
      >> > http://groups.yahoo.com/group/hobbicast
      >> >
      >> > For additional files and photos and off topic discussions
      >> > check out these two affiliated sites:
      >> > http://groups.yahoo.com/group/sandcrabs
      >> > http://groups.yahoo.com/group/Hobbicast1
      >> >
      >> > Please visit our sponsor: Budget Casting Supply
      >> > http://budgetcastingsupply.com/
      >> >
      >> > List Owner:
      >> > owly@...
      >> >
      >> >
      >> > Yahoo! Groups Links
      >> >
      >> >
      >> >
      >> >
      >> >
      >> >
      >>
      >
      >
      >
      >
      >
      >
      >
      > For discussion of Metal Casting and related issues
      > this list does not accept attachments.
      >
      > Files area and list services are at:
      > http://groups.yahoo.com/group/hobbicast
      >
      > For additional files and photos and off topic discussions
      > check out these two affiliated sites:
      > http://groups.yahoo.com/group/sandcrabs
      > http://groups.yahoo.com/group/Hobbicast1
      >
      > Please visit our sponsor: Budget Casting Supply
      > http://budgetcastingsupply.com/
      >
      > List Owner:
      > owly@...
      >
      >
      > Yahoo! Groups Links
      >
      >
      >
      >
      >
      >
      >
    • Show all 16 messages in this topic