Loading ...
Sorry, an error occurred while loading the content.

32283Re: Thermocouples ??s

Expand Messages
  • Michael
    Aug 29, 2004
    • 0 Attachment
      --- In hobbicast@yahoogroups.com, Leon Risenhoover <lrisen@d...> wrote:
      > ok I found my book on tc's
      > T =-320 to700fF
      > J=32to1400F
      > E=32 to1600F
      > K=32 to2000F
      > R or S =32 to2500F
      >
      >
      Are you sure about these? I was just looking at the Omega
      thermocouple chart on my wall and saw:
      T -454 to 752 deg F
      K -454 to 2501 deg F
      R -58 to 3214 deg F

      I know that my temp controller with type K reads to at least 2300F.

      Most of the thermocouple wires are listed as less range, but thats the
      insulation rating not the TC itself.

      Michael