Casey, what can you tell about the noise your diesel-burner is producing? Is it much louder than a gas-burner, as I expect it is? Secondly, am I right the...
I too have just built one and have also had problems. I have tried enlarging the air holes to 1/2" diameter but with only limited success so I am going to take...
My original burner was patterened after Oliver's design. However, I only have 10psi gas pressure available to me and there was no jet size that would work for ...
Hello Ray, This sounds like the problems I was having, as I was using a 6 psi regulator. I was advised to change from a .032" jet to a .039" one, and to use a...
Hi Gang - been a bit rushed off my feet. However - talking of Lancasters can't be ignored. I was very fortunate to have a 45 minute flight in "Son of...
... I assume there was some experimentation involved in the development of the original design to find the right balance between air and fuel flow. Now,...
17243
hobbicast@yahoogroups...
Jul 1, 2002 3:26 pm
Hello, This email message is a notification to let you know that a file has been uploaded to the Files area of the hobbicast group. File : /Diesel...
... mechanically ... written ... Done. I've put it in the same folder as the other images. It's pretty cool, actually, how the fuel adjustment works - the ...
... I don't have experience with any furnace, other than the one I made, so I can't compare it with anything. I can say ,though, that my diesel furnace is...
Very cool Bill !! That should help others to build one. Thank you for spending the time. Casey Brown ... this ... instructions ... debt. ... a ... how...
True enough, if I was installing one in my house or someone else was installing one in their house. However, here on base, we have to have contractors do this...
Saw this story on slashdot, and thought you guys would be interested. http://home.c2i.net/metaphor/mvpage.html He does better with his microwave than I do with...
I feel it is important to point out the mistakes I made in the construction of my torch,so that others can avoid them, and also to help determine if reducing...
Hey, this is really cool to cast liquid aluminum! This weekend, I finally finished my electrical furnace and gave it a try to melt down the 25 pound 356 Alu...
... would not happen to be made by Silv-o-lite would they? If so I just used a set for the first time in a streetrod SBC I am building, you can see them and...
17253
hobbicast@yahoogroups...
Jul 1, 2002 8:15 pm
Hello, This email message is a notification to let you know that a file has been uploaded to the Files area of the hobbicast group. File :...
As I discovered today, you are oh so right! However, Harbor Freight in the States do a little gizmo for filling little tanks from big tanks, and I know someone...
I wouldn't feel too bad if I were you. My burner is all machined out of solid brass stock and it doesn't turn off the water supply either. I haven't spent...
http://www.whiteriverfoundry.com/useful_links.htm cead mile failte! This email is a natural product. The slight variations in spelling and grammar enhance...
Matt, Nice Job! Great looking furnace and I like the "core" design. It much simplifies load bearing and insulation problems. Great us e of the castable and...
Whre on earth do you plan to find a 6.2L Cummins? The 6.2L is a GM product. The equivalent ligth truck engine is a 5.9L B series Cummins (6 cyl) or you can get...