Cross posted from the Gingery machines group. This message is for Paul Probus, Brian J. Bland, mike Turcotte, and anyone else interested in the Workbench...
I just finished my first pour of Silicon bronze. And it was a success!! Investment casting, using my own home brew investment, i poured 2 propellors, about 2...
I tried to melt copper tubing I had laying around the house today. Everything got to glowing a nice bright orange but no melt. How hot does this copper alloy...
My name is Christopher Richardson, I am from Deer Island NB Canada, (southern NB). Is there anyone here any where close to my area. I would be interested to...
Hi All, A bit off topic but I need a favour... an aquaintance has successfully sued a spammer! When I say successfully, I mean he's been awarded damages in a (...
I Need To Share This! Hey! My name is Karen and I am a blonde SWF that has been on the Internet dating scene for about a yeat without a lot of luck :-( I am...
Hi gang The yahoo marketing thing must(might) be US specific? (I think). Will other Aussies that have a .au on their e-mail address check their account info....
dreams can come true, even if they are small dreams.... :):):) READING THIS MESSAGE WILL CHANGE YOUR LIFE FOREVER !!!!!!PLEASE READ THIS ALL!!!!!!!!! !!!!IT...
Hello All, Roy drove up from Hope Hull Alabama today. Its great to meet people from this group face to face.He watched and ask questions as my helper and I...
I've been trying to contact Ray at hybridburners.com via email to purchase a 1 1/4" burner for a new furnace I'm attempting to build. Kinda a combination of...
edi, You need to adjust your rationale. After all, at 88, your uncle isn't going to be needing his back near as long as you will need yours.. Let him use it ...
Condolences, To our Brothers of the United Kingdom, on the passing of the "Brave and Gracious Lady", The Queen Mother. Our prayers are with you, on this most...
Hi there, Apologies if you already know this but I am passing on the following message. Unfortunately there appears to be a proposal by Yahoo to introduce ...
... Will was close on this one but I have learned a hell of a lot from people I swore were dumber than a springbound clock. Most everyone has something of...
Does anyone had a source for a circuit diagram for a homebuilt programmable electric furnace controller. This is more for heat treating stuff that has been...
Hi Guys, I was poking around looking for some way to contribute to this project when I ran across this site: http://www.5bears.com/ I you look under NEWS and...
So even if you never visit the web site and only receive email or digests, you still have an account, to which Yahoo has added a section called Marketing...
Check out the Photos section, I posted some pix from my little setup. I'm in a paperwork mood, I think I'll work on the FAQ a bit. Nearly done too. K'too...
Nice Guy, I got this from Rex a while back. Rex is in Georgia, his email is below. Ray in FLA ... Subject: Re: Burning question! Date: Wed, 02 Jan 2002...
Many of you have machine tool experience, so I would appreciate opinions. My drill press needs new bearings and a new spindle shaft. Instead of repairing it I...
I don't have a lot of money to spend on a comercialy built burner, what homemade burner is best? I want to melt mostly aluminum, but maby some iron. Thanks....
Hi, I did learn a lot from the time I spent with Charles. Everyone should watch someone with experience before trying their first pour. If anyone is close ...
I posted a few weeks back about this but did not see any replies. I am wondering if there are any rules of thumb about the thickness of furnace walls in an...
Many thanks to Ken Mayer and other list members for their advice on rust removal. I used electrolysis as Ken described. It removed all the rust from the ...
Yahoo is sticking it to you and I as bad as it can get.. Must be a better way.. but aint nothing free. This info came in from another list... I checked it out...
Hi, I need help concerning some half nuts I intend to cast, to replace the ones in the Gingery book. I am using a 3/4 x 6 tpi. acme screw and would like to...